Inconel Alloy 706 Pipe
video

Inconel Alloy 706 Pipe

Inconel 706 is a nickel-iron-chromium alloy is a precipitation-hardenable alloy which offers high mechanical strength in combination with good fabricability. Its characteristics are similar to those of Inconel718alloy except that it can be more readily fabricated and especially by machining.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 706 pipe in China. If you're going to wholesale high quality inconel alloy 706 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel Alloy 706 pipe is a highly engineered nickel-based alloy pipe widely used in demanding high temperature and corrosive environments.
Inconel 706 is mainly composed of nickel, chromium, iron and other elements, among which the nickel content is extremely high, which makes the alloy have excellent corrosion and oxidation resistance. The addition of chromium improves the stability of the alloy in oxidizing environments, while the addition of iron enhances the mechanical properties of the alloy.
This alloy also contains small amounts of niobium, molybdenum and titanium, which are added to enhance the strength and heat resistance of the alloy by forming stable precipitation phases.
High temperature performance and mechanical strength:
Inconel 706 is designed to withstand extreme temperature environments and has good creep resistance and fatigue strength, which enables it to operate at temperatures up to about 1100°C, suitable for aerospace and high temperature process applications.
The alloy not only exhibits excellent mechanical properties such as high tensile and yield strength at room temperature, but also maintains these properties in high temperature environments, thanks to its unique chemical composition and microstructure.

Mechanical Properties

Properties Conditions
T (°C) Treatment
Density (×1000 kg/m3) 7.8 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 515 25 annealed (sheet, strip) more
Yield Strength (Mpa) 275
Elongation (%) 40
Reduction in Area (%)  

Thermal Properties

Properties Conditions
T (°C) Treatment
Thermal Expansion (10-6/ºC) 17.5 0-100 more  
Thermal Conductivity (W/m-K) 16.2 100 more  
Specific Heat (J/kg-K) 500 0-100  

 

Inconel Alloy 706 pipeInconel Alloy 706 pipeInconel Alloy 706 pipe

Hot Tags: inconel alloy 706 pipe, China inconel alloy 706 pipe suppliers, inconel alloy blow molding process, inconel alloy cap fittings, high nickel corrosion alloys, Inconel Alloy 625 Pipe Fittings, inconel alloy decoder parts, inconel alloy control system parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry