Inconel 625LCF 693 Stainless Steel Pipe
video

Inconel 625LCF 693 Stainless Steel Pipe

Available Formats
GNEE Group offers Nickel Alloy Inconel 625LCF 693 in a variety of forms, including:
Bars
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 625lcf 693 stainless steel pipe in China. If you're going to wholesale high quality inconel 625lcf 693 stainless steel pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

inconel Products Application

Inconel 625LCF 693 stainless Pipe video

Used in the petrochemical processing industry to produce ammonia, methanol and hydrogen in synthetic natural gas production as thermowells, thermowell liners, pipe sleeves, baffles and valve assemblies, and reactors for syngas products.

inconel Material Specification

chemical composition of Inconel 625LCF

Element Composition (%)
S (Sulfur) ≤ 0.015%
C (Carbon) ≤ 0.03%
P (Phosphorus) ≤ 0.015%
Al (Aluminum) ≤ 0.40%
Co (Cobalt) ≤ 1.00%
Fe (Iron) ≤ 5.0%
Si (Silicon) ≤ 0.15%
Mn (Manganese) ≤ 0.50%
N (Nitrogen) ≤ 0.02%
Ti (Titanium) ≤ 0.40%
Nb + Ta (Niobium + Tantalum) 3.15% ~ 4.15%
Mo (Molybdenum) 8.0% ~ 10.0%
Cr (Chromium) 20.0% ~ 23.0%
Ni (Nickel) ≥ 58.0%

Inconel 693 Alloy Properties (Theoretical)

Compound Formula NiCrFeAl
Appearance Metallic powder or solid in various forms
Melting Point 1317 - 1367 °C
Boiling Point N/A
Density 7.77 g/cm3
Solubility in H2O N/A
Tensile Strength 882.6 MPa (hot-rolled, annealed plate)
Thermal Conductivity 9.10 W/m-K (23 °C)
Thermal Expansion 13.04 µm/m°C (100 °C)
Electrical Resistivity 1.169 µΩ·m
Specific Heat 484 J/kg·°C (100 °C)

Inconel 625LCF 693 stainless steel Pipe

Inconel 625LCF 693 steel Pipe priceInconel 625LCF 693 stainless Pipe dealer

INCONEL Alloy 625LCF (UNS N06626 / W. Nr. 2.4856) is a fatigue-resistant, bellows-quality version of INCONEL Alloy 625. Alloying, melting and processing are carefully designed and controlled to provide a plate product with optimum resistance to low cycle and thermal fatigue at temperatures up to 1200°F (650°C). The alloy provides high levels of performance in aircraft exhaust and automotive flexible coupling bellows, expansion joints in process or transportation piping, and other applications involving resistance to low cycle or thermal fatigue.
Alloy 693 has excellent oxidation resistance and corrosion resistance at high temperatures. It can withstand harsh environments such as high-temperature oxidation, sulfidation, and chlorination, and is not prone to corrosion and oxidation. This gives it long-term stability and reliability at high temperatures. 693 alloy maintains high strength and hardness at high temperatures and has excellent mechanical properties. It has good ductility, flexibility and impact properties, and is suitable for various high temperature application scenarios.

GNEE Group Factory Environment

Inconel 625LCF 693 Stainless Steel Pipe

Inconel 625LCF 693 Stainless Steel Pipe

Customer Case

customer visit

Inconel 625LCF 693 stainless steel Pipe factory

Inconel 625LCF 693 alloy Pipe suppliers

FAQ

 

 

 

 

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: What product information do I need to provide?
A: You need to provide the grade, width, thickness, coating and tonnage you need to purchase.

Q: About the product price of Inconel 625LCF 693 stainless steel Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Hot Tags: inconel 625lcf 693 stainless steel pipe, China inconel 625lcf 693 stainless steel pipe suppliers, inconel alloy reducer fittings, inconel alloy engine parts, inconel alloy gear parts, inconel alloy wire harness parts, inconel alloy plug fittings, inconel alloy fuel system parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry