Inconel 601GC 625LCF Pipe
video

Inconel 601GC 625LCF Pipe

Available Formats
GNEE Group offers Nickel Alloy Inconel 601GC 625LCF in a variety of forms, including:
Bars
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 601gc 625lcf pipe in China. If you're going to wholesale high quality inconel 601gc 625lcf pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

inconel Products Application

Inconel 601GC 625LCF ss Pipe video

Equivalent grades

• Inconel 625LCF
• UNS N06626
• W. Nr. 2.4856

inconel Material Specification

625LCF Pipe Chemical Composition (%)

Element Composition (%)
S (Sulfur) ≤ 0.015%
C (Carbon) ≤ 0.03%
P (Phosphorus) ≤ 0.015%
Al (Aluminum) ≤ 0.40%
Co (Cobalt) ≤ 1.00%
Fe (Iron) ≤ 5.0%
Si (Silicon) ≤ 0.15%
Mn (Manganese) ≤ 0.50%
N (Nitrogen) ≤ 0.02%
Ti (Titanium) ≤ 0.40%
Nb + Ta (Niobium + Tantalum) 3.15% ~ 4.15%
Mo (Molybdenum) 8.0% ~ 10.0%
Cr (Chromium) 20.0% ~ 23.0%
Ni (Nickel) ≥ 58.0%

Inconel 601GC Chemical Composition (%)

Element C Mn Fe S Ni Si Cr Zr N
Min - - - - 58.0 - 23.0 0.07 0.02
Max 1.0 1.0 15.0 0.015 63.0 1.0 25.0 0.25 0.07

Inconel 601GC 625LCF Pipe

Inconel 601GC 625LCF alloy Pipe priceInconel 601GC 625LCF material Pipe dealer

Inconel601GC is a version of Inconel601 that inhibits grain growth. Adding Zr and N can effectively inhibit the rate of grain growth of the alloy at high temperatures. Grain size stability at high temperatures is an important factor in achieving better performance and longer service life of the alloy.
Inconel 625LCF is a high performance nickel-based alloy material designed with a low carbon content alloy to achieve good strength and machinability properties. This material is widely used in high temperature and high pressure environments, mainly in aerospace, petrochemical, nuclear energy and other fields. Inconel 625LCF has excellent corrosion resistance and can withstand high-temperature corrosion from chlorides, sulfides and water, while having high fatigue and crack propagation resistance.

GNEE Group Factory Environment

Inconel 601GC 625LCF Pipe

Inconel 601GC 625LCF Pipe

Customer Case

customer visit

Inconel 601GC 625LCF material Pipe factory

Inconel 601GC 625LCF Pipe suppliers

FAQ

 

 

 

 

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: What product information do I need to provide?
A: You need to provide the grade, width, thickness, coating and tonnage you need to purchase.

Q: About the product price of Inconel 601GC 625LCF Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Hot Tags: inconel 601gc 625lcf pipe, China inconel 601gc 625lcf pipe suppliers, alloy tubing, inconel alloy spinning process, inconel alloy combustion chamber parts, inconel alloy actuator parts, Inconel 617 Super Stainless Pipe, inconel alloy connector parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry