Uns N08825 N08810 Alloy Pipe
Surface Finish: Polished, AP (Annealed and Pickled), BA (Bright and Annealed), MF
Straight Length: 65 feet (20 meters) maximum
Shape: Straight or "U" Bend
Surface Finish:
16 microinch Ra (ID 0.4 micron Ra)
4 microinch Ra (ID 0.1 micron Ra)
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n08825 n08810 alloy pipe in China. If you're going to wholesale high quality uns n08825 n08810 alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
incoloy Products Application
uns n08825 n08810 alloy Pipe video
Standard Specification of Incoloy 825 Tube
| Thickness | 0.3mm – 50 mm, SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS |
| Outer Diameter | 6.00 mm OD up to 914.4 mm OD, Sizes up to 24" NB |
| Type | Seamless / ERW / Welded / Fabricated / CDW |
| Form | Round Tubes, Square Tubes, Rectangular Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tubes |
| Length | Single Random, Double Random & Required Length |
| End | Plain End, Beveled End, Treaded. |
UNS N08810 Alloy Pipe information
| Category | Details |
|---|---|
| Brand Type | INCOLOY alloy 810 |
| Product Range | Rod, wire, ring, forging, shaft, sheet, strip, band, tape, pipe, offsets and flanges, various industrial custom parts upon customer request |
| Machining | Lathe machining, milling, grinding, deep drilling (max length: 9.8 meters) |
| Heat Treatment | Normalization, annealing, tempering, quenching, quench and temper, holding, shell hardening, carburizing |
incoloy Material Specification
chemical composition of Incoloy 825 (Nickel Alloy 825 / UNS N08825)
| Element | Composition (wt. %) |
|---|---|
| Nickel (Ni) | 38.00 – 46.00 |
| Chromium (Cr) | 19.50 – 23.50 |
| Iron (Fe) | 22.00 min (minimum) |
| Titanium (Ti) | 0.06 – 1.20 |
| Molybdenum (Mo) | 2.50 – 3.50 |
| Copper (Cu) | 1.50 – 3.00 |
| Carbon (C) | 0.05 max (maximum) |
| Manganese (Mn) | 1.0 max |
| Sulfur (S) | 0.03 max |
| Silicon (Si) | 0.5 max |
| Aluminum (Al) | 0.2 max |
Chemical composition of INCOLOY 810 alloy:
| C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
|---|---|---|---|---|---|---|
| 0.25 | 0.8 | 0.9 | 21 | 32 | ||
| Mo | Al | Cu | Nb | Ti | V | Ce |
| 0.5 | ||||||
| N | Co | Pb | B | Other | ||


825 nickel alloy, also called INCOLOY825 alloy, UNS N08825 is its international brand. Due to its high nickel, high molybdenum and copper design, it has good corrosion resistance and is widely used in air pollution control, chemical and petrochemical products, food processing, Nuclear industry, offshore oil and gas mining, ore processing, petroleum refining, steel pickling and waste treatment and other industries with corrosion-resistant applications.
N08810/No8810 high carbon alloy has a carbon content between 0.05 and 0.10. It is mainly used for temperatures above 600 degrees. It has the characteristics of coarse grains, high creep strength, good mechanical properties and corrosion resistance. Superheaters, reheaters, high-temperature heating, conversion and cracking furnace tubes in chemical industry, electric power, and petrochemical industry.
GNEE Group Factory Environment
Uns N08825 N08810 Alloy Pipe

Customer Case
customer visit


FAQ
Q: Can I get your best price?
A: Our goal is to provide you with the best price and excellent quality assurance in the long run. Please leave your contact information to get the best quote, we will provide you with the best solution as soon as possible.
Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. Or if the goods are not in stock, it is 15-20 days, depending on the quantity.
Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.
Q: About the product price of uns n08825 n08810 alloy Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Hot Tags: uns n08825 n08810 alloy pipe, China uns n08825 n08810 alloy pipe suppliers, alloy for construction, Inconel Alloy 617 Seamless Pipe, incoloy stainless pipe, Incoloy Metal Tubing, alloy for flanges, alloy for etching baths
You Might Also Like
Send Inquiry