Inconel 825 Round Bar
Chromium: 19.50 - 23.50
Iron: 22.00 min
Titanium: 0.06 - 1.2
Molybdenum: 2.50 - 3.50
Copper: 1.50-3.00
Carbon: 0.05 max
Manganese: 1.0 max
Sulfur: 0.03 max
Silicon: 0.5 max
Aluminum: 0.2 max
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 825 round bar in China. If you're going to wholesale high quality inconel 825 round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
In the oil and gas industry, the two most important nickel alloys are Inconel 625 and Incoloy 825. lncoloy 825 is an austenitic nickel-iron-chromium-molybdenum-copper alloy containing high levels of chromium, nickel, copper and molybdenum to provide high levels of corrosion resistance to both moderately oxidizing and moderately reducing environments. This balance of alloying elements grants this alloy exceptional resistance to both chloride stress corrosion cracking, as well as crevice corrosion and general corrosion. It is the high level of nickel in combination with the amount of molybdenum and copper in this nickel alloy produces substantially improved corrosion resistance in a corrosive environment such as reducing environments compared to stainless steel. The addition of titanium in this alloy also helps to stabilize the alloy against intergranular corrosion. Chloride stress corrosion cracking is a type of localised intergranular corrosion on materials that are put under tensile strength, in high temperatures and in an environment that includes oxygen and chloride ions such as seawater.
As an austenitic, nickel alloy, the material is ductile over a wide range of temperatures from cryogenic to well in excess of 1000 °F (538 °C). Fabricability is typical for a nickel alloy, with the material readily formable and weldable by a variety of techniques.
Product Parameter
|
Element |
Min % |
Max % |
|
Ni |
38.00 |
46.00 |
|
Co |
– |
2.00 |
|
Cu |
1.50 |
3.00 |
|
Cr |
19.50 |
23.50 |
|
Mo |
2.50 |
3.50 |
|
Al |
– |
0.20 |
|
C |
– |
0.05 |
|
Si |
– |
0.50 |
|
Mn |
– |
1.00 |
|
S |
– |
0.03 |
|
Ti |
0.60 |
1.20 |
Application
• Chemical processing components
• pollution control
• oil and gas recovery
• pickling tank parts
• nuclear fuel processing
PHYSICAL PROPERTIES
Density: 0.294 lbs/in3, 8.14 g/cm3
Specific Heat, (32 - 212 ° F), Btu/lb•° F, (0 - 100 °C), J/kg•°C: 0.105 (440)
Mean Coefficient of Thermal Expansion: in/inl° F (mm/ml°C):
70 - 212 ° F (20 - 100 °C): 7.7 x 10-5 (13.9)
Thermal Conductivity: BTU/h-ft-° F (W/m-° K) 70 ° F (21 °C): 6.4 (11.1)
Modulus of Elasticity: ksi (MPa)
28.4 x 103 (196 x 103) in tension
Permeability at 70 ° F (21 °C) H = 200 Oersted :
Annealed : 1.005
Melting Point: 2500 - 2550 ° F (1370 - 1400 °C)
Our Company

38000㎡ workshop and 200+ emplovees to meet your huge demands.
Packing & Delivery

Customer Visit

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide
FAQ
Q:About product prices?
A:Prices vary from period to period due to cyclical changes in the price of raw materials.
Q: Are you a factory or trading company?
A: We are professional manufacturer, and our company also is a very professional a trade company for steel products.We can provide a wide range of steel products.
Q:What do your factory do regarding quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.
Q: Can I get samples before order ?
A: Yes, of course. Usually our samples are free. we can produce by your samples or technical drawings.
Hot Tags: inconel 825 round bar, China inconel 825 round bar suppliers, alloy for gasket materials, alloy for strengthening, lncoloy 825 plate, alloy for insulation materials, iron based alloy, alloy for nitridation resistance