800 925 330 Incoloy external polishing Tube
video

800 925 330 Incoloy external polishing Tube

Incoloy 800 alloy seamless pipe

Size: 4 - 219 mm
Thickness: 0.5 - 20 mm
Length: single layer, double layer, random length and cut to length
Incoloy 800 alloy welded pipe

Size: 5.0 - 1219.2 mm
Thickness: 0.5 - 20 mm
Length: single layer, double layer, random length and cut to length
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 800 925 330 incoloy external polishing tube in China. If you're going to wholesale high quality 800 925 330 incoloy external polishing tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

800 925 330 Incoloy Tube information

 

800 925 330 incoloy pipe video

GNEE STEEL GROUP supplies 800 925 330 Incoloy Tube for you

 

GNEE STEEL GROUP supplies incoloy 800

UNS Number N08810/N08811

Other common names: Alloy 800, Alloy 800H, Inconel® 800, Alloy 800HT

ASTM B 409, B 408, B 407, B 564

ASME SB407 Code Case 1325, SB 408, SB409

W. NR. 1.4958, 1.4959

What forms of Incoloy 800H/HT does GNEE STEEL offer?
Plates
Rods
Tubes (welded and seamless)
Fittings
Elbows, tees, nipples, returns, caps, crossheads, reducers, fittings, etc.
Wire

PRODUCT FORM SIZE RANGE FROM SIZE RANGE TO
Alloy 800 pipe 0.5 in 8 in
Alloy 800 tube 12 mm 260 mm
Alloy 800 pipe fittings 0.5 in 8 in
Alloy 800 flanges 0.5 in 8 in

GNEE STEEL GROUP supplies incoloy 925

• Incoloy alloy 925
• UNS N09925
• JIS NCF 925

PRODUCT FORM SIZE RANGE FROM SIZE RANGE TO
Alloy 925 pipe 0.5 in 8 in
Alloy 925 tube 12 mm 260 mm
Alloy 925 pipe fittings 0.5 in 8 in
Alloy 925 flanges 0.5 in 8 in

We can provide Incoloy 925 in various forms according to your customization, such as: 

Incoloy Alloy 925 Bar Incoloy Alloy 925 Sheet&Plate
Incoloy Alloy 925 Welded Pipe&Tube Incoloy Alloy 925 Seamless Pipe&Tube
Incoloy Alloy 925 Pipe Fittings Incoloy Alloy 925 Fasteners
Incoloy Alloy 925 Forgings Incoloy Alloy 925 Flanges
Incoloy Alloy 925 Coil Incoloy Alloy 925 wire

GNEE STEEL GROUP supplies incoloy 300

• Incoloy 330
• UNS N08330
• W.Nr. 1.4886
• RA330

Product Form Standard
Bars and shapes ASTM B511
Billets and bars ASTM B512
Seamless pipes and tubes ASTM B535, B829
Weld pipes and tubes ASTM B546, B710, B739
Plates, sheets and strips ASTM B536
Welded fittings ASTM B366
Forging SAE AMS 5716
800 925 330 Incoloy Tube Specification

Alloy 800 (UNS N08800) Chemical Composition, %

Ni Cr Fe C Al Ti Al+Ti

30.0-35.0

19.0-23.0

39.5 min

.10 max

.15-.60

.15-.60

.30-1.20

925 Incoloy Tube Chemical Composition

  Cr Ni Mo Co Nb (+Ta) Ti W Cu C Mn N Si P S Fe Al
Min 19.5 42 2.5   0.08 1.9   1.5               0.1
Max 22.5 46 3.5   0.5 2.4   3 0.025 1   0.35 0.02 0.003 Bal 0.5

330 Incoloy Tube Chemical Composition

Element Content (%)
Iron, Fe 43
Nickel, Ni 34-37
Chromium, Cr 17-20
Manganese, Mn ≤2
Others Remainder

800 925 330 incoloy tube

800 925 330 incoloy seamless tube suppliers800 925 330 iincoloy pipe dealer

The Alloy 800 Series (Incoloy 800, 800H, and 800HT) are nickel-iron-chromium superalloys that provide high-temperature strength and resistance to oxidation, carburization, and other types of high-temperature corrosion. Alloy 800 (UNS N08800), Alloy 800H (UNS N08810) and Alloy 800HT (UNS N08811) have the same nickel, chromium and iron contents, but differ in the combined levels of titanium and aluminum (0.85 to 1.2%) to ensure optimal high temperature characteristic.
Incoloy 08925 (also known as "Alloy 925"), known as UNS N925, is a precipitation-hardening iron-nickel-chromium alloy with the addition of molybdenum, copper, titanium, and aluminum. The alloy provides excellent resistance to general corrosion, pitting corrosion, crevice corrosion and stress corrosion cracking in many aqueous environments, including those containing sulfides and chlorides.
Incoloy 330 is a non-austenitic heat and corrosion resistant alloy that offers a combination of strength and resistance to carburization, oxidation and thermal shock. This alloy is designed for use in high temperature industrial environments where the combined effects of carburization and thermal cycling and good electrical resistance are necessary, such as in applications in the heat treatment industry. Carburization and oxidation resistance to approximately 2100°F are enhanced by the silicon content in the alloy.

GNEE Group Factory Environment

800 925 330 external polishing Tube

800 925 330 Incoloy external polishing Tube

800 925 330 Incoloy Tube process & size

800 925 330 Incoloy Tube process & size

800 925 330 Incoloy Tube

800 925 330 Incoloy Tube

 

Gnee Steel Customer Case

customer visit

800 925 330 Incoloy Tube

 

FAQ

Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.

Q: What are your payment terms?
A: Payment <=1000USD, 50% in advance. Payment >=1000USD, 30% T/T in advance, balance before shipment. or negotiable

Q: About the product price of 800 925 330 incoloy tube?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

contact us

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

Hot Tags: 800 925 330 Incoloy external polishing Tube, China 800 925 330 Incoloy external polishing Tube suppliers, alloy for neurology baths, alloy for fasteners, alloy for digital light processing baths, alloy for extraction baths, alloy for turning tools, high temperature alloys

Send Inquiry

whatsapp

Phone

E-mail

Inquiry