Incoloy Alloy 909 Seamless Pipe
video

Incoloy Alloy 909 Seamless Pipe

Incoloy Alloy 909 seamless pipe is a testament to advanced materials engineering, offering a blend of high-temperature performance, corrosion resistance, and mechanical integrity. Its application in numerous high-temperature and corrosive environments underscores its importance in industries where robust materials are paramount. Proper utilization of this alloy can significantly enhance the efficiency and lifespan of critical components, reducing maintenance costs and improving operational reliability.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 909 seamless pipe in China. If you're going to wholesale high quality incoloy alloy 909 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

INCOLOY alloy 909 (UNS N19909) is a nickel-iron-cobalt alloy whose outstanding characteristics are a constant low coefficient of thermal expansion, a constant modulus of elasticity, and high strength. The alloy is strengthened by a precipitation-hardening heat treatment made possible by additions of niobium and titanium.

Physical Properties

Density g/cm3 8.19
lb/in.3 0.296
Melting Range °F 2540 - 2610
°C 1395 - 1430

Mechanical Properties

Condition & Size Tensile Strength Yield Strength
(0.2% Offset)
Elongation Reduction of Area Hardness
MPa, min MPa, min %, min %, min HB
Solution Treated ... ... ... ... 277 max
Aging Treated 1172 862 10 15 331min

 

Incoloy Alloy 909 seamless pipeIncoloy Alloy 909 seamless pipeIncoloy Alloy 909 seamless pipe