Incoloy Alloy 926 seamless pipe offers a combination of excellent corrosion resistance and good mechanical properties, making it suitable for a variety of demanding industrial applications. Its ability to perform well in challenging environments has made it a preferred material choice for industries where reliability and longevity are critical.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 926 seamless pipe in China. If you're going to wholesale high quality incoloy alloy 926 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

926 is an austenitic stainless steel alloy has a similar chemical composition with 904L alloy, its nitrogen content is 0.2%, molybdenum content is 6.5%. Molybdenum and nitrogen content significantly increased the resistance of pitting and crevice corrosion in the halide media.Meantime, nickel and nitrogen not only ensures the stability of metallographical, but also reduce separating intergranular trend in the thermal process or welding process better than the nitrogen content of nickel alloy. 926 has particular corrosion resistance in the chloride ions medium due to the excellent local corrosion resistance and 25% nickel alloy content.A variety of experiments in the 10000-70000ppm of Chloride concentration, PH 5-6, 50-68ºC operating temperature of the slurry of limestone FGD system show that, after a 1-2 year trial period, 926 alloy without pitting and crevice corrosion.926 in other chemical media also has good corrosion resistance in the high temperature and high concentration of media, including sulfuric acid, phosphoric acid, acid gas, sea water, salt and organic acids.926 is the material that choosed for BAM directory Chapter 6 of "dangerous goods storage and transportation containers norms" by Berlin, Germany's national Institute for Materials Research and Testing (BAM) . In addition, in order to have the best corrosion resistance only when the material is in the right state of metallurgy and guarantee clean conditions.

Physical Properties

Density g/cm3 8.03
lb/in.3 0.29
Melting Range °F 2410 - 2550
°C 1320 - 1400

Mechanical Properties

Condition & Size Tensile Strength Yield Strength
(0.2% Offset)
Elongation Reduction of Area Hardness
MPa, min MPa, min %, min %, min Rockwell
Solution annealed 650 295 35 ... ...

 

Incoloy Alloy 926 seamless pipeIncoloy Alloy 926 seamless pipeIncoloy Alloy 926 seamless pipe

Hot Tags: incoloy alloy 926 seamless pipe, China incoloy alloy 926 seamless pipe suppliers, corrosion resistant material, incoloy pipe steel, alloy for flexible manufacturing baths, alloy products, precision alloy rod, alloy for mixing baths

Send Inquiry

whatsapp

Phone

E-mail

Inquiry