Incoloy 925 28 Alloy Small diameter Pipe
video

Incoloy 925 28 Alloy Small diameter Pipe

Incoloy 925 Tube, 925 Incoloy Pipe, Incoloy 925 Welded Tube, Incoloy Alloy 925 ERW Tube, Incoloy 925 EFW Tube, Incoloy Alloy 925 Welded Round Tube Manufacturer.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 925 28 alloy small diameter pipe in China. If you're going to wholesale high quality incoloy 925 28 alloy small diameter pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy 925 28 Small diameter Pipe introduce

925 28 Alloy Small diameter Pipe

Incoloy 925 28 Alloy Small diameter PipeIncoloy 925 28 Alloy Small diameter Pipe

Incoloy 925 is the perfect choice, this alloy consists mainly of nickel, chromium and iron, which has excellent strength and durability. Incoloy 925 pipes are available in a variety of sizes and shapes. They are usually round or square, with different diameters and wall thicknesses. Incoloy 925 pipe is an alloy of nickel, chromium and iron, which combines excellent corrosion resistance, strength, ductility and formability.
Incoloy 925 pipe is an alloy of nickel, chromium and cobalt, which has excellent corrosion resistance in a variety of environments. It is a fully austenitic stainless steel that can be hardened by cold working. Incoloy 925 pipe has excellent resistance to pitting, crevice corrosion and stress corrosion cracking. It also has excellent resistance to sulfuric acid, hydrochloric acid and alkaline, organic and saline solutions.

Alloy 28 is a high alloy multi-purpose stainless steel suitable for highly corrosive environments. This grade of steel has enhanced resistance to strong acid corrosion. Moreover, it has good resistance to intergranular corrosion and stress corrosion cracking in a wide range of environments. Its excellent resistance to crevice corrosion and pitting corrosion and excellent weldability make it ideal for numerous applications. Hence, Alloy 28 Tubes are widely used in many industrial sectors.
Gnee Steel is one of the largest manufacturers, suppliers and stockists of premium industrial products in the world. Alloy 28 Tubes is one of the wide range of products they offer to buyers. The offered range of products is reasonably priced and easy to source. Buyers can customize the products in various specifications including wall thickness, size, length, shape, ends, type, etc. as per customer requirements.

What is the advantages of Incoloy 925 Pipes & Tubes?

Incoloy 925 Pipes & Tubes offer superior corrosion resistance in various environments, making them ideal for many applications. They feature excellent resistance to pitting, crevice corrosion, and stress corrosion cracking. They are highly resistant to sulfuric & hydrochloric acids, alkaline solutions, organic acids & salt solutions.

What are the Benefits of Incoloy 925 Pipes & Tubes?

Incoloy 925 Pipes & Tubes offer many benefits, making them an ideal choice for many applications. These include superior corrosion resistance to a broad range of acidic, alkaline & salt solutions and organic acids. It provides excellent resistance to pitting, crevice corrosion & stress corrosion cracking.

Incoloy 925 Pipes & Tubes Specification

Specifications ASTM B983 / ASME SB983
Dimensions ASTM, ASME and API
Size Range 15"NB – 150"NB
Outer Diameter 6.35 mm OD upto 254 mm OD in 0.6 TO 20 mm thickness.
Schedule SCH 10, SCH20, SCH30, SCH40, STD, SCH60, XS, SCH80, SCH120, SCH140, SCH160, XXS
Type Seamless / ERW / Welded / Fabricated / LSAW Pipes
Length Single Random, Double Random & Cut Length
Form Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tube

925 Incoloy Alloy Pipes Chemical Composition

Grade C Mn Si Fe S Cr Cu Ni
925 min. – – – 22.0 – 19.5 1.5 42.0
max. – – – – – 22.5 3.0 46.0

Inconel 925 Pipe / Tubes Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.08 g/cm3 1311°C-1366 °C 685 MPa 271 MPa 56%

Alloy 28 Pipes Chemical Composition

Element Alloy 28
C ≤ 0.02
Si 0.70
Mn 2.00
P 0.03
S 0.01
Cr 26.0-28.0
Mo 3.00-4.00
Ni 30.0-32.0
N ≤ 0.11
Cu 0.70-1.50

Alloy 28 Pipes Mechanical & Physical Properties

Element Alloy 28
Tensile strength Rm
N/mm²
500-750
0.2% Yield strength Rp
≥ N/mm²
220
Elongation A5
≥ %
35/30
Hardness HB 30
≤ HB
230
Modulus of elasticity
kN/mm²
195

GNEE Group Factory Environment

metal 925 28 Alloy Small diameter Pipe

Incoloy 925 28 Alloy Small diameter Pipe

GNEE Group Product Packaging

Incoloy metal 925 28 Alloy Small diameter Pipe

Incoloy 925 28 Alloy Small diameter Pipe

FAQ

Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Q: Will the Test Certificate meet EN10204 3.1/3.2?
A: We will provide Original Mill Test Certificate certified to EN10204 3.1/3.2 for products in stock or further processing needed.
Q: How long is your delivery time?
A: Generally it is 2-5 days if the goods are in stock or it will need 7-20 days if the goods need to be customized.
Q: Do you provide samples Is it free or extra?
A: Yes, we could offer free samples.

Hot Tags: incoloy 925 28 alloy pipe, China incoloy 925 28 alloy pipe suppliers, alloy for etching baths, alloy materials, alloy for additive manufacturing baths, alloy for vat photopolymerization baths, welded alloy pipe, alloy for evaporation baths

Send Inquiry

whatsapp

Phone

E-mail

Inquiry