Incoloy Alloy 020 Pipe
video

Incoloy Alloy 020 Pipe

INCOLOY alloy 020 (UNS N08020) has excellent corrosion resistance in chemical environments containing sulfuric acid, and useful resistance to environments containing chlorides, nitric acid, and phosphoric acid. Other uses include the production of gasoline, solvents, explosives, inorganic and organic chemicals, pharmaceuticals, and food and synthetic materials. INCOLOY alloy 020 is readily fabricated to produce mixing tanks, heat exchangers, process piping, pickling equipment, pumps, valves, fasteners and fittings. Applications for alloy 020 requiring resistance to aqueous corrosion are essentially the same as those for INCOLOY alloy 825.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 020 pipe in China. If you're going to wholesale high quality incoloy alloy 020 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy Alloy 020 is a nickel-based alloy that is widely used in various industrial fields for its excellent corrosion resistance and good mechanical properties. This alloy is designed to resist a variety of corrosive environments and maintain high strength and stability, even in extreme temperature conditions.

Physical Properties

Density g/cm3 8.08
lb/in.3 0.292
Specific Heat Btu/lb-°F 0.12
J/kg-°C 500
Thermal Conductivity at 200°F (93°C) Btu-in/ft2-h-°F 85
W/m-°C 12.3
Electrical Resistivity ohm circ mil/ft 651
μΩ-m 1.08
Young's Modulus (70°F) 103 ksi 28
GPa 193
Shear Modulus (70°F) 103 ksi 11
GPa 76
Coefficient of Expansion 77-212°F, 10-6 in/in•°F 8.2
25-100°C, μm/m•°C 14.7

Mechanical Properties

Tensile Strength ksi 90
MPa 620
Yield Strength (0.2% Offset) ksi 45
MPa 300
Elongation % 40

 

Incoloy Alloy 020 pipeIncoloy Alloy 020 pipeIncoloy Alloy 020 pipe