INCOLOY® alloy 27-7MO (UNS S31277) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-austenitic stainless steels. In many environments alloy 27-7MO offers resistance approaching that of much more highly alloyed materials such as INCONEL alloys 625, 22, and C-276. Alloy 27-7MO products typically contain 27% nickel, 22% chromium, 7.2% molybdenum, and 0.34% nitrogen. Its limiting chemical composition is presented in Table 1. The alloy's content of nickel and nitrogen produce a stable austenitic structure. By virtue of its content of molybdenum, chromium, and nitrogen, alloy 27-7MO offers excellent resistance to pitting and crevice corrosion. The nickel, nitrogen, and molybdenum provide resistance to reducing media while a high content of chromium offers resistance to oxidizing media. Alloy 27-7MO performs well in mixed acid environments, especially those containing oxidizing and reducing acids.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 27-7mo seamlesspipe in China. If you're going to wholesale high quality incoloy alloy 27-7mo seamlesspipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy Alloy 27-7MO seamless pipe is a type of pipe made from Incoloy Alloy 27-7MO, which is a nickel-chromium-iron alloy known for its excellent corrosion resistance and high-temperature strength. This alloy contains approximately 72% nickel, 16% chromium, and 8% iron, along with small amounts of other elements such as manganese, silicon, and carbon. Incoloy Alloy 27-7MO is particularly resistant to oxidation and corrosion in high-temperature environments, making it suitable for use in a variety of industrial applications.

Seamless pipes are manufactured by hot working a solid billet in a piercing mill or a rotary forging press to create a hollow tube, which is then further processed through a series of rolling and stretching operations to achieve the desired dimensions and wall thickness. The seamless construction ensures that the pipe has no weld seams, which can be potential weak points in the material.

INVENTORY

PRODUCT FORM SIZE RANGE FROM SIZE RANGE TO
Alloy 27-7MO pipe 0.5 in 8 in
Alloy 27-7MO tube 12 mm 260 mm
Alloy 27-7MO pipe fittings 0.5 in 8 in
Alloy 27-7MO flanges 0.5 in 8 in

 

Tensile Data

Mechanical Property Requirements

 

Ultimate Tensile

Yield Strength (0.2% OS)

Elong.

R/A

Hardness

Min

120 KSi

60 KSi

50

 

Rb 95

Max

         

Min

827 MPa

414 MPa

     

Max

         

Incoloy Alloy 27-7MO seamlesspipeIncoloy Alloy 27-7MO seamlesspipeIncoloy Alloy 27-7MO seamlesspipe