Inconel 718SPF Super Alloy Pipe
video

Inconel 718SPF Super Alloy Pipe

Available Formats
GNEE Group offers Nickel Alloy Inconel 718 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 718spf super alloy pipe in China. If you're going to wholesale high quality inconel 718spf super alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 718SPF Super Alloy Pipe introduce

Inconel 718SPF Super Alloy Pipe

Inconel 718SPF Super Alloy PipeInconel 718SPF Super Alloy Pipe

Super alloys or high performance alloys have an ability to function at temperatures above 540ºC (1000ºF) with deformation resistance and high surface stability. As they have good oxidation and creep resistance, super alloys can be commonly forged, rolled to sheet or produced in various shapes. Iron-base, nickel-base and cobalt-base alloys are the major types of super alloys. Nickel-base and cobalt-base super alloys may be cast or wrought based on its composition or application. The iron-base super alloys are generally wrought alloys with stainless steel technology. These alloys can be strengthened by precipitation hardening, work hardening and solid-solution hardening.

Our company is engaged in the production and trade of various Inconel 686 718SPF Super Alloy Pipe, high-performance, high-precision special-shaped steel pipes and seamless pipes. We have established business relationships with customers in more than 20 countries and regions. Details such as payment method, delivery time and minimum quantity can be negotiated based on the order.

Due to its high temperature strength, excellent corrosion resistance and easy processability at 700°C, Inconel718 alloy can be widely used in various high-demand situations.

1.Steam turbine

2. Liquid fuel rocket

3.Cryogenic engineering

4.Acidic environment

5. Nuclear Engineering

Inconel 718SPF Super Alloy Pipe Specification
Element Min % Max %
Ni Balance Balance
Cr 19.0 23.00
Mo 15.0 17.0
W 3.0 4.4
Ti 0.02 0.25
Fe 1.0
C 0.01
Mn 0.75
S 0.02
Si 0.08
P 0.04

Physical Properties

The physical properties of Inconel 718SPF are given in the following table.

Properties Metric Imperial
Density 8.19 g/cm³ 0.296 lb/in³

Mechanical Properties

The mechanical properties of Inconel 718SPF are displayed in the following table.

Properties Metric Imperial
Tensile strength 1120 MPa 162000 psi
Yield strength (at 0.2%) 827 MPa 120000 psi
Modulus of elasticity 205 GPa 29700 ksi
Poissons ratio 0.284 0.284
Elongation at break 31% 31%
Hardness, Rockwell C 24 24

GNEE Group Factory Environment

Inconel 718SPF Super Alloy Pipe

Inconel 718SPF Super Alloy Pipe


GNEE Group Product Packaging

Inconel 718SPF Super Alloy Pipe

Inconel 718SPF Super Alloy Pipe

FAQ

Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.

Hot Tags: inconel 718spf super alloy pipe, China inconel 718spf super alloy pipe suppliers, alloy for tissue engineering baths, alloy for cleaning baths, alloy for molds, alloy for oil and gas, alloy for creep resistance, alloy for intelligent manufacturing baths

Send Inquiry

whatsapp

Phone

E-mail

Inquiry