Incoloy 330
video

Incoloy 330

INCOLOY® alloy 330 (UNS N08330 / W. Nr. 1.4886) is an austenitic alloy with good high-temperature strength and corrosion resistance. It has a solid solution composition and is not hardenable by heat treatment. Its high nickel and chromium provide good resistance to oxidation and carburization. Its oxidation resistance is enhanced by the silicon content.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 330 in China. If you're going to wholesale high quality incoloy 330 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

INCOLOY® alloy 330 (UNS N08330 / W. Nr. 1.4886) is an austenitic alloy with good high-temperature strength and corrosion resistance. It has a solid solution composition and is not hardenable by heat treatment. Its high nickel and chromium provide good resistance to oxidation and carburization. Its oxidation resistance is enhanced by the silicon content.

The alloy's strength and oxidation resistance at elevated temperatures make it a useful material for industrial heating furnaces; for muffles, retorts, conveyor systems, baskets and boxes, and various fixtures.

Corrosion Resistance

INCOLOY® alloy 330 offers a high level of corrosion resistance, articularly to oxidation, carburization and nitridation. In aqueous environments, the alloy's chromium content provides resistance to oxidizing onditions while its nickel content imparts resistance to reducing conditions. The high nickel also gives INCOLOY alloy 330 good resistance to chloride-ion stress-corrosion cracking.

Main Standards

ASTM B535

Seamless Pipe & Tube

ASTM B829

Seamless Pipe & Tube

ASTM B710

Welded Pipe

ASTM B739

Welded Tube

ASTM B546

Electric Fusion Welded Tube

ASTM B366

Welded Fittings

ASTM B511

Bars and Shapes

ASTM B512

Billets and Bars

ASTM B536

Plate, Sheet and Strip

SAE AMS 5716

Bars, Wire, Forgings and Rings

SAE AMS 5592

Plate, Sheet and Strip

Chemical Composition

Data Sheet

Physical Properties

Density g/cm3 8.08
lb/in.3 0.292
Melting Range °F 2520 - 2590
°C 1380 - 1420
Specific Heat 32-212°F Btu/lb•°F 0.11
0-100°C J/kg•°C 460
Permeability at 70°F (21°C) and 200 oersted (15.9 kA/m) Annealed 1.02
Poisson's Ratio at 70°F (20°C)   0.340

Mechanical Properties

Form and Condition Tensile Strength Yield Strength
(0.2% Offset)
Elongation
ksi MPa ksi MPa %
Plate, hot-rolled & annealed 80-85 552-586 30-43 207-296 40-45
Sheet, cold-rolled & annealed 80-90 552-621 32-42 221-290 35-45
Rod, hot-finished & annealed 80-90 552-621 35-45 241-310 38-45

More +

FAQ

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

 

Hot Tags: incoloy 330, China incoloy 330 suppliers, alloy for creep resistance, alloy for inspection baths, lncoloy 901 Alloy Steel Bar, alloy for dentistry baths, alloy for waste treatment baths, alloy for evaporation baths

Send Inquiry