Incoloy 907 Steel Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 907 steel pipe in China. If you're going to wholesale high quality incoloy 907 steel pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Incoloy 907 Steel Pipe
Incoloy 907 926 Steel Pipe is a versatile material that can be used in many industrial fields: 1. Fire protection systems, seawater purification systems, hydraulic and perfusion piping systems in marine engineering. 2. Bleaching tank in cellulose pulp production. 3. Polished rods in corrosive oil wells. 4. Hose systems in marine engineering. 5. Pipelines, joints, gas flow systems, etc. in acid gas production. 6. Components in the flue gas desulfurization system. 7. Evaporators, heat exchangers, filters, mixers, etc. in phosphoric acid production. 8. Sulfuric acid separation and condensation system.
Incoloy 907 926 Steel Pipe Specification
| Elements | Content (%) |
|---|---|
| Iron, Fe | 42 |
| Nickel, Ni | 38 |
| Cobalt, Co | 13 |
| Niobium, Nb | 4.7 |
| Titanium, Ti | 1.5 |
| Silicon, Si | 0.15 |
| Aluminum, Al | 0.03 |
Hot Tags: incoloy 907 steel pipe, China incoloy 907 steel pipe suppliers, alloy stainless pipe, alloy for aging, alloy for prosthetics baths, nickel alloy, alloy for creep resistance, Incoloy 27 7MO Alloy Pipe