Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy ds pipe in China. If you're going to wholesale high quality incoloy alloy ds pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Incoloy Alloy DS pipe is a type of pipe made from Incoloy Alloy DS, a nickel-based superalloy that is highly resistant to corrosion and oxidation. This alloy is particularly useful in applications where materials are exposed to extreme temperatures and harsh chemical environments.Incoloy Alloy DS pipe is commonly used in the chemical processing, petroleum refining, and nuclear industries. It is also used in the production of acids, such as hydrochloric and sulfuric acid, and in the handling of other corrosive substances.
Physical Properties
| Density | g/cm3 | 7.86 | |
|---|---|---|---|
| lb/in.3 | 0.284 | ||
| Melting Range | °F | 2426 - 2552 | |
| °C | 1330 - 1400 | ||
Alloy DS Pipe and Tubes Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel DS | 8 | 1430°C | 550-750 | 230 | 30 % |
Inconel DS Pipes & Tubes Equivalent Grades
| STANDARD | WERKSTOFF NR. | UNS |
| Inconel DS | 1.4862 | N08330 |