Incoloy 926
video

Incoloy 926

Alloy Name: Incoloy 926
UNS: N08926, W.Nr.1.4529
Forms: Plate, sheet, strip, seamless/welded pipe, bar, fitting
Matrix type: Super‑austenitic solid‑solution strengthened alloy
Key features: Excellent pitting / crevice / SCC resistance in chloride‑rich media
Applicable standards: ASTM A240, B625, B677, B366
Delivery condition: Solution‑annealed
Mandatory test: PMI, UT, inter‑granular corrosion test
Typical industries: Seawater desalination, marine, FGD, chemical & phosphoric‑acid equipment
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 926 in China. If you're going to wholesale high quality incoloy 926 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy 926 Product Introduction

 

 

Incoloy 926 (N08926) nickel-based alloy contains 14.0-18.0% Cr and 24.0-26.0% Ni. It is a nickel-based alloy containing titanium and aluminum, with enough chromium to form and maintain a sufficient scale of chromium oxide to protect it under high temperature conditions. Incoloy 926 is more heat resistant than typical chrome-nickel stainless steel such as 304. The high nickel contained within gives it better oxidation resistance than the standard 18-8 type stainless steel. Its oxidation resistance is equivalent to (if not higher than) the higher-grade alloys used at temperatures up to 1900 degrees Fahrenheit (1038 °C).

 

Incoloy 926 Product Parameter
 

 

Chemical Composition:

Grade % C Si Mn P S Cr Ni Cu Mo N
N08926 MIN - - - - - 19 24 0.5 6 0.15
  MAX 0.02 0.5 2 0.03 0.011 21 26 1.5 7 0.7

 

Physical Properties:

Density Melting Point
8.1 g/cm³ 1320–1390 °C

 

Mechanical Properties:

Alloy State Tensile Strength Rm (N/mm²) Yield Strength (MPa, N/mm²) Elongation A5 (%)
Annealed ≥650 ≥295 ≥35

 

Incoloy 926 Executive Standard

 

 

Products ASTM Standards
Plates ASTM A240
Pipe Fittings ASTM A312

 

Incoloy 926 Application
 

 

1) Reverse osmosis seawater desalination device, seawater heat exchanger, capacitor tube, etc.;

2) Pulp and paper industry, various bleaching devices, etc.;

3) Resin production device, reaction containers for drugs, piping, etc.;

4) Firefighting systems, seawater purification systems, hydraulic and perfusion piping;

5) Systems in marine engineering;

6) Hose system in marine engineering;

7) Pipes, joints, airflow systems, etc. in the production of acid gases;

8) Parts in flue gas desulfurization systems;

9) Evaporators, heat exchangers, filters, mixers, etc. in the production of phosphoric acid;

10) Sulfuric acid separation and condensation system;

11) Cooling-water pipe systems in Power plant;

12) Storage tank for corrosive chemical transportation;

13) Halogen acid catalyzed organic production equipment;

14) Others.

 

Incoloy 926 Feature
 

 

Main features of Incoloy 926 (N08926) nickel base alloy are listed as below.

1) Incoloy 926 (N08926) features high resistance to pitting and crevice corrosion in halide media and acidic media containing H2S.

2) It can effectively resist chloride ion stress corrosion cracking (SCC) in practical applications.

3) It is resistant to various corrosions in the usual oxidation and reduction environments.

4) It has enhanced mechanical performance in contrast to Cronifer 1925 LC-Alloy 904L.

5) It features improved metallurgical stability compared with Ni18 alloys.

6) It is certified to the application of pressure vessel manufacturing (VdTUV-196 ~ 400 °C and ASME certification).

 

Our Company
 

 

product-750-416

38000㎡ workshop and 200+ emplovees to meet your huge demands.

 

Packing & Delivery
 

 

product-750-750

 

Customer Visit
 

 

product-750-750

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide

 

FAQ
 

 

Q: What is your terms of payment ?

A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable.

Q: What are the advantages of your company ?

A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.

Q: How many coutries you already exported ?

A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.

Q: Can you provide sample ?

A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

 

Hot Tags: incoloy 926, China incoloy 926 suppliers, alloy for semiconductors, alloy for crystallization baths, high temperature alloys, alloy for electron beam melting baths, alloy for acid resistance, alloy for actuators

Send Inquiry

whatsapp

Phone

E-mail

Inquiry