825 800H 926 Incoloy Tube
video

825 800H 926 Incoloy Tube

Incoloy 825 is a titanium stabilized fully austenitic nickel iron chromium alloy with added copper and molybdenum. Incoloy 825 is a general-purpose engineering alloy that resists acid and alkali metal corrosion in both oxidizing and reducing environments.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 825 800h 926 incoloy tube in China. If you're going to wholesale high quality 825 800h 926 incoloy tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

825 800H 926 Incoloy Tube Description

825 800H 926 incoloy pipe video

GNEE STEEL GROUP supplies 825 800H 926 Incoloy Tube for you

 

GNEE STEEL GROUP supplies incoloy 825

UNS Number N08825

Other common names: Alloy 825, Inconel 825

What forms of Incoloy 825 does GNEE STEEL offer?

Plates
Plate
Rods
Tubes (welded and seamless)
Fittings
Elbows, tees, nipples, return tubes, caps, crossheads, reducers, fittings, etc. Welding wire (AWS classification: ERNiFeCr-1 and ENiCrMo-3)
Wire

 

GNEE STEEL GROUP supplies incoloy 800H

UNS Number N08810/N08811

Other common names: Alloy 800, Alloy 800H, Inconel 800, Alloy 800HT

ASTM B 409, B 408, B 407, B 564

ASME SB407 Code Case 1325, SB 408, SB409

W. NR. 1.4958, 1.4959

 

What forms of Incoloy 800H/HT does GNEE STEEL offer?
Plates
Rods
Tubes (welded and seamless)
Fittings
Elbows, tees, short ends, return pipes, caps, crossheads, reducers, pipe fittings, etc.
Wire

 

GNEE STEEL GROUP supplies incoloy 926

UNS N08926

Werkstoff Nr. 1.4529

EN X1 NiCrMoCuN25-20-7

GNEE STEEL GROUP supplies incoloy 926 Form

Standard

Metal Type

UNS N08800 / N08810 / N08811

Bar

ASTM B408

Wire

 

Sheet

ASTM B409

Plate

ASTM B409

Fitting

ASTM B366

Forging

ASTM B564

Weld Wire

 

Weld Electrode

 

 

825 800H 926 Incoloy Tube Specification

Alloy 825 (UNS N08825) Chemical Composition, %

Ni Fe Cr Mb Cu Ti C Mn S Si Al

38.0-46.0

22.0 min

19.5-23.5

2.5-3.5

1.5-3.0

.6-1.2

0.05 max

1.0 max

0.03 max

0.5 max

0.2 max

Alloy 800H (UNS N08800) Chemical Composition, %

Ni Cr Fe C Al Ti Al+Ti

30.0-35.0

19.0-23.0

39.5 min

.10 max

.15-.60

.15-.60

.30-1.20

926 Incoloy Tube Chemical Composition

Grade Ni% Cr% Mo% Fe% C% Mn% Si% Cu% N% P% S%
Incoloy 926 24.0-26.0 20.0-21.0 6.0-7.0 Bal. Max 0.02 Max 1.0 Max 0.5 0.5-1.5 0.15-0.25 Max 0.03 Max 0.01

825 800H 926 Incoloy Tube

825 800H 926 incoloy seamless Tube suppliers825 800H 926 Incoloy ss Tube dealer

Incoloy 825 is a titanium stabilized fully austenitic nickel iron chromium alloy with added copper and molybdenum. Incoloy 825 is a general-purpose engineering alloy that resists acid and alkali metal corrosion in both oxidizing and reducing environments.
The Cr content in Incoloy 800H (NO8810) nickel-based alloy is usually 15-25%, the nickel content is 30-45%, and it contains small amounts of aluminum and titanium. Compared with Incoloy 800 alloy, the carbon content is controlled from less than or equal to 0.1% to 0.05-0.1%, which better improves the strength of the steel.
926 is an austenitic stainless steel with a chemical composition similar to 904L alloy. Compared with 904L, the nitrogen content of 926 has been increased to about 0.2%, and the molybdenum content is about 6.5%. The increased content of nitrogen and molybdenum significantly improves its resistance to pitting and crevice corrosion in halide media.

GNEE Group Factory Environment

Incoloy Tube

p20241206133940c7eca

825 800H 926 Incoloy Tube process & product size

825 800H 926 Incoloy Tube process & product size

825 800H 926 Incoloy Tube

825 800H 926 Incoloy Tube

 

Customer Case

customer visit

825 800H 926 Incoloy Tube

 

FAQ

Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.

Q: What are your payment terms?
A: Payment <=1000USD, 50% in advance. Payment >=1000USD, 30% T/T in advance, balance before shipment. or negotiable

Q: About the product price of 825 800H 926 Incoloy Tube?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

contact us

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

Hot Tags: 825 800h 926 incoloy tube, China 825 800h 926 incoloy tube suppliers, alloy for neurology baths, Incoloy Metal Tubing, precision alloy rod, alloy for shafts, alloy for acid resistance, alloy for high pressure applications

Send Inquiry

whatsapp

Phone

E-mail

Inquiry