Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ams 5589 gh4169 seamless tubes for gas turbine in China. If you're going to wholesale high quality ams 5589 gh4169 seamless tubes for gas turbine made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
From land-based gas turbines to advanced marine propulsion systems, our Gnee Steel AMS 5589 GH4169 seamless steel tubing provides the critical thermal stability required for long-cycle operation. We understand that downtime is unacceptable in power generation. Therefore, our tubing undergoes rigorous manufacturing processes to withstand thousands of start-stop cycles without structural degradation.
Click to get bulk pricing for GH4169 gas turbine tubes
AMS 5589 GH4169 Seamless Tubes for Gas Turbine description

The AMS 5589 standard defines high-performance seamless GH4169 (Inconel 718) nickel alloy tubing designed for aerospace and gas turbine applications, offering superior creep resistance and high strength up to 1300°F (704°C). These tubings also exhibit excellent corrosion resistance and high tensile strength, making them ideal for hot-end turbine components and fluid piping.
Request a GH4169 pipe price quote
GH4169 aircraft engine fuel pipe Description
| Parameter | Description |
|---|---|
| Specification | AMS 5589 (Aerospace Material Specification) |
| Material | GH4169 (UNS N07718 / Inconel 718) |
| Product Form | Seamless Cold Worked Tube |
| Application | Gas Turbine Engines (combustor liners, bleed air systems, fuel manifolds, cooling lines) |
| Design Requirements | High temperature strength, oxidation resistance, thermal fatigue resistance, creep strength |
| Applicable Standards | AMS 5589, AMS 5590, ASTM B983, ASME SB983 |
Note: AMS 5589 is the primary aerospace specification for Inconel 718 seamless tubing used in gas turbine and high-temperature aircraft applications. The material is produced by vacuum induction melting (VIM) followed by vacuum arc remelting (VAR).
AMS 5589 GH4169 Tubes Specification
AMS 5589 GH4169 Tubes Chemical Composition
| Ni | Cr | Nb+Ta | Mo | Ti | Al | Cu | Fe |
| 50.0-55.0 | 17.0-21.0 | 4.75-5.50 | 2.80-3.30 | 0.65-1.15 | 0.20-0.80 | ≤ 0.3 | Bal. |
Mechanical properties of GH4169 gas turbine tubes
| Test Condition | Tensile Rm (MPa) | Yield Rp0.2 (MPa) | Elongation A5 (%) | Reduction of Area (%) |
|---|---|---|---|---|
| High Temp (650°C) | ≥ 1000 | ≥ 850 | ≥ 15 | ≥ 20 |
Click to download the GH4169 alloy PDF file now
Standard pipe diameter for GH4169 gas turbine applications
| OD (in) | OD (mm) | Wall (in) | Wall (mm) | Weight (lb/ft) | Weight (kg/m) | Typical Gas Turbine Application |
|---|---|---|---|---|---|---|
| 0.125 | 3.18 | 0.016 | 0.41 | 0.013 | 0.019 | Instrumentation, small cooling lines |
| 0.125 | 3.18 | 0.020 | 0.51 | 0.016 | 0.024 | High-pressure instrumentation |
| 0.188 | 4.78 | 0.020 | 0.51 | 0.025 | 0.037 | Control lines, low-flow cooling |
| 0.188 | 4.78 | 0.028 | 0.71 | 0.034 | 0.051 | Bleed air sensing, general cooling |
| 0.188 | 4.78 | 0.035 | 0.89 | 0.042 | 0.063 | High-pressure cooling lines |
| 0.250 | 6.35 | 0.020 | 0.51 | 0.034 | 0.051 | Fuel return, balance lines |
| 0.250 | 6.35 | 0.028 | 0.71 | 0.047 | 0.070 | Fuel supply, general cooling |
| 0.250 | 6.35 | 0.035 | 0.89 | 0.058 | 0.086 | Main cooling air, fuel manifolds |
| 0.250 | 6.35 | 0.049 | 1.24 | 0.079 | 0.118 | High-pressure air supply |
| 0.313 | 7.95 | 0.028 | 0.71 | 0.060 | 0.089 | Combustor cooling lines |
| 0.313 | 7.95 | 0.035 | 0.89 | 0.074 | 0.110 | Turbine cooling supply |
| 0.313 | 7.95 | 0.049 | 1.24 | 0.102 | 0.152 | High-flow cooling manifolds |
| 0.375 | 9.53 | 0.028 | 0.71 | 0.073 | 0.109 | Main bleed air lines |
| 0.375 | 9.53 | 0.035 | 0.89 | 0.090 | 0.134 | Turbine cooling supply |
| 0.375 | 9.53 | 0.042 | 1.07 | 0.107 | 0.159 | High-pressure cooling mains |
| 0.375 | 9.53 | 0.049 | 1.24 | 0.124 | 0.185 | Extreme pressure cooling |
| 0.500 | 12.70 | 0.035 | 0.89 | 0.122 | 0.182 | Main cooling air manifolds |
| 0.500 | 12.70 | 0.049 | 1.24 | 0.168 | 0.250 | High-volume cooling supply |
| 0.500 | 12.70 | 0.065 | 1.65 | 0.218 | 0.324 | Main bleed air headers |
| 0.625 | 15.88 | 0.035 | 0.89 | 0.154 | 0.229 | Large cooling ducts |
| 0.625 | 15.88 | 0.049 | 1.24 | 0.213 | 0.317 | Combustor case cooling |
| 0.625 | 15.88 | 0.065 | 1.65 | 0.278 | 0.414 | High-volume main supply |
| 0.750 | 19.05 | 0.049 | 1.24 | 0.258 | 0.384 | Main cooling air headers |
| 0.750 | 19.05 | 0.065 | 1.65 | 0.337 | 0.502 | Large engine cooling mains |
| 0.750 | 19.05 | 0.083 | 2.11 | 0.422 | 0.628 | Heavy-duty cooling systems |
| 1.000 | 25.40 | 0.065 | 1.65 | 0.458 | 0.681 | Main engine air supply |
| 1.000 | 25.40 | 0.083 | 2.11 | 0.578 | 0.860 | High-volume air distribution |
GH4169 is the most commonly used gas turbine tube size
| Rank | OD (in) | OD (mm) | Wall (in) | Wall (mm) | Usage Frequency | Typical Application Area |
|---|---|---|---|---|---|---|
| 1 | 0.250 | 6.35 | 0.035 | 0.89 | Very High | Bleed air, cooling, fuel manifolds |
| 2 | 0.188 | 4.78 | 0.028 | 0.71 | Very High | Sensing lines, control cooling |
| 3 | 0.375 | 9.53 | 0.035 | 0.89 | High | Turbine cooling, bleed air mains |
| 4 | 0.250 | 6.35 | 0.028 | 0.71 | High | Fuel supply, general cooling |
| 5 | 0.500 | 12.70 | 0.049 | 1.24 | Medium | Main cooling air manifolds |
| 6 | 0.313 | 7.95 | 0.035 | 0.89 | Medium | Combustor cooling, turbine supply |
| 7 | 0.125 | 3.18 | 0.020 | 0.51 | Medium | Instrumentation, small cooling |
| 8 | 0.188 | 4.78 | 0.020 | 0.51 | Medium | Low-flow cooling, return lines |
| 9 | 0.500 | 12.70 | 0.035 | 0.89 | Medium | Main cooling air, large manifolds |
| 10 | 0.375 | 9.53 | 0.042 | 1.07 | Low | High-pressure cooling mains |
GH4169 Tube Size Guide for Gas Turbine Applications
| Application Area | Recommended OD (in) | Recommended Wall (in) | Operating Temp (°C) | Pressure (psi) |
|---|---|---|---|---|
| Cooling Air Lines (Low Flow) | 0.125 – 0.188 | 0.016 – 0.020 | 300-500 | 200-500 |
| Cooling Air Lines (General) | 0.188 – 0.250 | 0.020 – 0.028 | 400-600 | 500-1,000 |
| Cooling Air Lines (High Flow) | 0.250 – 0.375 | 0.028 – 0.035 | 500-700 | 1,000-2,000 |
| Main Cooling Manifolds | 0.500 – 0.750 | 0.049 – 0.065 | 500-650 | 500-1,500 |
| Bleed Air Lines (Low Pressure) | 0.250 – 0.375 | 0.028 – 0.035 | 400-600 | 200-500 |
| Bleed Air Lines (High Pressure) | 0.313 – 0.500 | 0.035 – 0.049 | 500-650 | 500-1,500 |
| Main Bleed Air Headers | 0.500 – 1.000 | 0.049 – 0.083 | 500-650 | 300-800 |
| Fuel Manifolds | 0.188 – 0.313 | 0.028 – 0.035 | 50-150 | 500-3,000 |
| Fuel Supply Lines | 0.250 – 0.500 | 0.028 – 0.049 | 50-150 | 500-5,000 |
| Combustor Cooling | 0.250 – 0.375 | 0.035 – 0.049 | 600-700 | 1,000-2,000 |
| Turbine Cooling Supply | 0.313 – 0.500 | 0.035 – 0.049 | 500-650 | 500-1,500 |
| Instrumentation / Sensing | 0.125 – 0.188 | 0.016 – 0.020 | 300-600 | 100-500 |
| Control Lines (Hydraulic/Pneumatic) | 0.188 – 0.250 | 0.020 – 0.028 | 100-300 | 1,000-3,000 |
| Case Cooling Lines | 0.375 – 0.625 | 0.035 – 0.049 | 400-600 | 300-800 |
Contact us to customize GH4169 products to fit your project dimensions
Advantages of GH4169 Fuel System Piping
Even in land-based gas turbines, the fuel system is the most critical component. GH4169's superior performance is reflected in the following aspects:
Anti-coking performance: Its smooth inner wall and high-temperature stability prevent fuel from coking within the piping, ensuring stable burner performance.
Pressure pulsation stability: GH4169 maintains its elastic modulus under high-frequency pressure waves, preventing fatigue failure caused by vibration.
Weld joint integrity: Its excellent resistance to strain-aging cracking makes it an ideal choice for the complex welded manifolds of gas turbine combustors.
Main Applications of GH4169 Nickel Alloy Tubes
Gas turbine: Internal fuel piping, cooling air piping, and high-strength fasteners.
Steam turbine: High-pressure steam delivery piping and heat exchanger piping.
Marine propulsion: Exhaust system and fuel injection piping for high-performance ship engines.
Nuclear power: Core structural components and instrumentation piping.




GH4169 Non-destructive Testing (NDT) Requirements for Tubes
Gnee Alloy as a trusted supplier, Gnee Alloy adheres to a "zero-defect" principle. Every GH4169 seamless pipe undergoes a rigorous inspection process before shipment.
| Test Method | Requirement | Standard | Acceptance Criteria |
|---|---|---|---|
| Ultrasonic Testing (UT) | 100% (for wall ≥ 0.5mm) | ASTM E213 | No defects exceeding 5% wall |
| Eddy Current Testing (ET) | 100% (for thin wall) | ASTM E426 | No relevant indications |
| Hydrostatic Test | 100% | ASME Section VIII | 1.5× working pressure, no leakage |
| Pneumatic Test | As specified | – | For clean gas service |
| Visual Inspection | 100% | ASTM E543 | No surface defects |




GNEE Group GH4169 superalloy Packaging
GNEE Group GH4169 superalloy Packaging

Contact us to choose your preferred packaging and shipping method
Why Choose Gnee Steel's GH4169 Seamless Pipe
Stable Metallurgical Properties: Our VIM + ESR dual-melting process ensures a uniform microstructure, resulting in high fatigue life and creep rupture resistance.
Supply Chain Security: We offer price-locking solutions and annual supply agreements to help you manage material cost fluctuations in long-term projects.
Professional Logistics Services: We have extensive experience shipping high-value alloy batches to Southeast Asia, and the Middle East, and provide comprehensive customs clearance and compliance support.

GH4169 certificate
FAQ
Q: Do you offer long-term supply contracts for OEMs?
A: Yes. We specialize in supporting large-scale projects through annual supply agreements. We offer price-lock options to protect our clients from raw material (Nickel/Niobium) price volatility, ensuring stable project budgeting.
Q: Are your tubes compatible with high-temperature steam environments?
A: Absolutely. GH4169 (Inconel 718) provides excellent resistance to steam, high-purity water, and various industrial gases, even in the presence of chlorides, making it superior to 300-series stainless steels.
Q: Can you provide oversized tubes for heavy-duty turbine casings?
A: Yes, we have the capability to produce seamless pipes up to 219mm OD with wall thicknesses up to 25mm, meeting the needs of heavy structural energy components.
Hot Tags: ams 5589 gh4169 seamless tubes for gas turbine, China ams 5589 gh4169 seamless tubes for gas turbine suppliers, engineering alloy, product alloy, Monel K500 Nickel Alloy Pipe, durable alloy, tool alloy, aerospace alloy
You Might Also Like
Send Inquiry