Hastelloy B2 Alloy Steel Coil
video

Hastelloy B2 Alloy Steel Coil

Hastelloy B2 coil specifications
Width: 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc.
Length: 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc.
Thickness: 0.3mm to 120mm
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy b2 alloy steel coil in China. If you're going to wholesale high quality hastelloy b2 alloy steel coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy B2 Steel Coil introduce

Hastelloy B2 Coil

Hastelloy B2 Alloy Steel CoilHastelloy B2 Alloy Steel Coil

Gnee Steel offers Hastelloy B2 Sheets and Coils, which are manufactured under the guidance of our experienced experts who ensure that advanced techniques and latest tools are used in the production process. In addition, Hastelloy B2 Sheets also offer excellent resistance to pitting and stress corrosion cracking. Hastelloy B2 Coils control other alloying elements such as chromium and iron and solve other issues related to machinability. Molybdenum is the main alloying component of Hastelloy B2 Sheets and Coils, which provides important corrosion resistance to reducing environments. Hastelloy B2 Perforated Coils are molybdenum-nickel alloys that have strong corrosion resistance to reducing environments such as sulfuric acid, hydrogen chloride gas, phosphoric acid and acetic acid. B2 Sheets are also available in customized sizes and shapes to our customers. Gnee Steel is one of the well-known suppliers and distributors of B2 Coils, always providing excellent services. The picture shows the largest batch of B2 Sheets and Coils known to date, which is a thin sheet lining for the exposed environment of a utility flue gas desulfurization unit. Due to its durability and corrosion resistance, B2 alloy perforated coils were selected as an alternative in FRP fans for handling radioactive and hazardous waste incineration. A practical problem of Hastelloy UNS N10665 plates being susceptible to intergranular corrosion is the heat affected zone of welds.

Hastelloy B2 Coils Specifications

Specifications ASTM / ASME SB333
Size 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Thickness 0.1mm to 12 mm Thk
Form Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Chemical Composition of Hastelloy B2 Sheets, Plates & Coils

Grade C Mn Si S Co Ni Cr Fe Mo P
B2 0.010 max 1.00 max 0.08 max 0.03 max 2.50 max 50.99 min* 14.50 – 16.50 4.00 – 7.00 15.00 – 17.00 0.04 max

Mechanical properties of Hastelloy B2 Sheets, Plates & Coils

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy B2 8.89 g/cm3 1370 °C (2500 °F) Psi – 1,15,000 , MPa – 790 Psi – 52,000 , MPa – 355 40 %

GNEE Group Factory Environment

Hastelloy B2 Alloy Coil

Hastelloy B2 Alloy Steel Coil

GNEE Group Product Packaging

B2 Alloy Steel Coil

Hastelloy B2 Alloy Steel Coil

FAQ

Question1: Are you a trading company or manufacturer?
Answer: We're manufacturer.

Question2: Could you help to design the product?

Answer: Yes, we have excellent R&D team, OEM/ODM orders are all welcome.

Question3: Could you supply samples?

Answer: Yes, wecould supply samples according to your requirement.

Hot Tags: Hastelloy B2 Alloy Steel Coil, China Hastelloy B2 Alloy Steel Coil suppliers, Alloy Steel 600 plate, Ni36CrTiAl Plate, Monel 400 Alloy Steel Sheet, 2 4668 Nickel Alloy Steel Coil, Cold Rolled Inconel 625 Alloy Seamless Pipe, Nickel Alloy Coil B2

Send Inquiry

whatsapp

Phone

E-mail