Hastelloy B2 Coil Specifications
Specifications: ASTM B333 / ASME SB333
Width: 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc.
Length: 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc.
Thickness: 0.3mm to 120mm
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel alloy polished b2 coil in China. If you're going to wholesale high quality nickel alloy polished b2 coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

 

Nickel Alloy Polished B2 Coil Description

Chemical composition of MonelR405 nickel-copper alloy strip

 

Gnee Steel Nickel Alloy Polished B2 Coil

The chemical composition of Hastelloy B2 coil mainly includes nickel, chromium, molybdenum and a small amount of iron, tungsten and other elements. The combination of these elements gives the material excellent corrosion resistance and high temperature strength. Among them, nickel provides good corrosion resistance, chromium enhances the corrosion resistance of the material in an oxidizing environment, and molybdenum improves the corrosion resistance of the material in a reducing environment. The addition of elements such as iron and tungsten further improves the strength and hardness of the material. Hastelloy B2 coil has good processing properties and can be used for hot and cold processing.

Hastelloy B2 Coils Specification

Specifications : ASTM B333 / ASME SB333

Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc

Length : 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc

Thickness : 0.3 mm to 120 mm

Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Finish : Hot rolled (HR), Cold rolled coils (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Form : Plain Coils, Shim Coils, Strip, Flats, Blank (Circle), Ring (Flange)

 

Nickel Alloy Polished B2 Coil specifications

Chemical Composition of Hastelloy B2 Coils

Grade C Mn Si S Co Ni Cr Fe Mo P
Hastelloy B2 0.02 max 1.0 max 0.1 max 0.03 max 1.0 max Bal 1.0 max 2.0 max 26 – 30 0.04 max

Hastelloy B2 Coils Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy B2 9.2 g/cm3 1370 °C (2500 ºF) Psi – 1,10,000 , MPa – 760 Psi – 51000 , MPa – 350 40 %

Nickel Alloy Coil B2 Factory Environment

Nickel Alloy Coil B2

Nickel Alloy Coil Polished B2

Coil Polished B2 Packaging

Coil Polished B2

Nickel Alloy Coil Polished B2

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel is a company specializing in the production of various nickel-based alloys, nickel 201, nickel202, hastelloy c-276, hastelloy c-22, hastelloy b, hastelloy c-4, Inconel alloy 600, Inconel 625, Inconel 718, Inconel x-750, incoloy alloy 800, incoloy 800H/HT, incoloy 825, monel alloy 400, monel k500 and high temperature alloy materials. It specializes in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, electric power, automobile, nuclear energy and other fields, and can provide customized alloy material solutions according to customer needs. If you need to know the alloy material price consultation or provide customized alloy material solutions, you are welcome to contact us at any time to get a quote at ss@gneesteel.com

Hot Tags: Nickel Alloy Polished B2 Coil, China Nickel Alloy Polished B2 Coil suppliers, Ni36CrTiAl Plate, Nickel Alloy Coil B2, Monel 400 Alloy Steel Sheet, Cold Rolled Inconel 625 Alloy Seamless Pipe, Uns N06600 Alloy tubing, 2 4668 Nickel Alloy Steel Coil

Send Inquiry

whatsapp

Phone

E-mail

Inquiry