Model NO. Nm450 NM400 NM500 Standard ASTM, AISI, GB, JIS, DIN, BS Certification ISO Surface Treatment Blackface Technique Hot Rolled Special Use Wear Resistant Steel Stock Stock Product Name Nm4500 Hot Rolled Steel Plate Keyword Aabrasion Resistant Steel Packing Ply Wood Pallets
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nm450 nm400 nm500 abrasion resistant steel in China. If you're going to wholesale high quality nm450 nm400 nm500 abrasion resistant steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nm450 Nm400 Nm500 Abrasion Resistant Steel

Product Description

Hot Rolled Wear Abrasion Resistant Steel Plate NM450





Chemical component

Chemical Composition (%) of NM450 Wear Resistant Steel
C Si Mn P S Al Cr+Mo+Ni
0.10-0.40 0.20-0.40 1.0-2.0 ≤0.015 ≤0.003 ≥0.02 <1.2


Machanical property

Mechanical Properties of NM450 Wear Resistant Steel
Thickness/mm ReL /MPa Rm /MPa A/% Hardness/ HBW10/3000 Impact -20ºC /J
8 1250 1460 16 445 40
12 1290 1470 17 462 43
20 1370 1450 17 473 42
25 1230 1480 16.5 465 43

 

GB Specification Wear Resistant Steel Mechanical Properties

Grade C Si Mn P S Cr Mo Ni Bt
NM360 ≤0.25 ≤0.70 ≤1.60 ≤0.025 ≤0.015 ≤0.80 ≤0.50 ≤0.50 0.0005-0.006
NM400 ≤0.30 ≤0.70 ≤1.60 ≤0.025 ≤0.010 ≤1.00 ≤0.50 ≤0.70 0.0005-0.006
NM450 ≤0.35 ≤0.70 ≤1.70 ≤0.025 ≤0.010 ≤1.10 ≤0.55 ≤0.80 0.0005-0.006
NM500 ≤0.38 ≤0.70 ≤1.70 ≤0.020 ≤0.010 ≤1.20 ≤0.65 ≤1.00 0.0005-0.006
NM550 ≤0.38 ≤0.70 ≤1.70 ≤0.020 ≤0.010 ≤1.20 ≤0.70 ≤1.00 0.0005-0.006
NM600 ≤0.45 ≤0.70 ≤1.90 ≤0.020 ≤0.010 ≤1.50 ≤0.80 ≤1.00 0.0005-0.006

GB Specification Abrasion Resistant Steel Chemical Composition

Grade Tensile Strength Elongation Impact test(-20°) HBW
NM360 ≥1100 ≥12 ≥24 330-390
NM400 ≥1200 ≥10 ≥24 370-430
NM450 ≥1250 ≥7 ≥24 420-480
NM500 / / / ≥470
NM550 / / / ≥530
NM600 / / / ≥570