Alloy 602CA / 2.4633

2.4633 is a high carbon chromium-iron-nickel alloy which also contains additives of microalloy elements titanium, zirconium and aluminum, and yttrium. Alloy 602CA is characterized by: - excellent high temperature creep properties - excellent fatigue resistance in the HCF and LCF mode - extraordinary oxidation resistance at high temperatures and under cyclic conditions.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 602ca / 2.4633 in China. If you're going to wholesale high quality alloy 602ca / 2.4633 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

2.4633 is a high carbon chromium-iron-nickel alloy which also contains additives of microalloy elements titanium, zirconium and aluminum, and yttrium. Alloy 602CA is characterized by:

- excellent high temperature creep properties

- excellent fatigue resistance in the HCF and LCF mode

- extraordinary oxidation resistance at high temperatures and under cyclic conditions.

 

Material Data Sheet

Material Designation 2.4633
Alloy Alloy 602CA
EN Material Symbol NiCr25FeAIY
UNS N 06025
Trademark Nicrofer® 6025 HT
VdTÜV Data Sheet 540
Norm DIN EN 10302

Main fields of application of alloy 602CA

Alloy 602 is versatile. Typical applications of Alloy 602CA are, i.e.:

- Rotary kiln and shaft

- Furnace rollers / Oven Parts

- nozzles

- pipe supports

- Components in the exhaust gas purifying catalyst of automobiles

- Reformers in the chemical and petrochemical industry

- Hydrogen production

- Heater plugs

Chemical composition of alloy 602CA

C Si Mn P S Cr
≤ % ≤ % ≤ % ≤ % ≤ % %
0.15-0.25 0.5 0.5 0.02 0.01 24.0-26.0
Al Zr Ti Cu Fe Y Ni
% % % ≤ % ≤ % ≤ % %
1.8-2.4 0.01-0.1 0.1-0.2 0.1 8.11 0.05-0.12 Rest

Characteristics of alloy 602CA

Temperature Range High-Temperature Range
Density 7.9 g/cm³
ISO-V notch impact toughness lengthwise 69 J/cm² at room temperature
  across 56 J/cm² at room temperature

Filler metal (for welding with alloy 602CA)

Alloy 602CA can be welded using 2.4649 and DIN EN ISO 18274: S Ni 6025 as filler metal

Covered electrodes: DIN EN ISO 1412: E Ni 6025

UNS W86025

AWS A5.11: ENiCrFe-12

Delivery program

Sheets / Plates mm

2 - 20

Coils mm

2

Bars / Billets dia. mm

20 - 35

With short delivery time:

plates or sheets, tubes, flanges, forged or die-cut rings and round blanks, elbows, T-fittings, reductions, screws, nuts or washers according to your request. According to your individual wishes, we are able to cut our material with our plasma- or water jet cutter. Our material is stocked in superformats of 2000x6000mm. Cut to size on request.

 

 

FAQ

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Kazakhstan, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: alloy 602ca / 2.4633, China alloy 602ca / 2.4633 suppliers, Uns N06600 Alloy tubing, Nickel Alloy Coil B2, Cold Rolled Inconel 625 Alloy Seamless Pipe, Alloy Steel 600 plate, Monel 400 Alloy Steel Sheet, 2 4668 Nickel Alloy Steel Coil

Send Inquiry

whatsapp

Phone

E-mail

Inquiry