Product Introduction
Hastelloy N alloy is a nickel-based high-temperature alloy material used in molten salt reactors. It has excellent corrosion resistance, resistance to neutron radiation and good high-temperature mechanical properties. However, the reactor outlet temperature reached 750°C, exceeding the allowable temperature of Hastelloy N alloy of 704°C, which means that the alloy cannot operate stably in a 750°C molten salt environment for a long time. Therefore, there is an urgent need to optimize Hastelloy N alloy to meet the requirements of higher temperature molten salt reactors.
Hastelloy N
The chemical composition of Hastelloy N is given in the following table.
Element
Content (%)
Nickel, Ni
71
Molybdenum, Mo
16
Chromium, Cr
7
Iron, Fe
≤ 5
Silicon, Si
≤ 1
Manganese, Mn
≤ 0.80
Tungsten, W
≤ 0.50
Aluminum, Al + Titanium, Ti
≤ 0.50
Copper, Cu
≤ 0.35
Cobalt, Co
≤ 0.20
Carbon, C
≤ 0.080
Application
Used in molten fluoride salt containers and other fields
1 Industrial and aviation turbines.
2 Industrial furnace components, support rollers, grids, ribbons and radiant tubes.
3 Spiral tubes in petrochemical furnaces.
4 Spiral tubes in petrochemical furnaces.
5 High-temperature gas cools nuclear reactors.