Hastelloy B-3 B-2 Pipe
video

Hastelloy B-3 B-2 Pipe

HASTELLOY C276 is a Nickel-chromium-molybdenum wrought alloy that is considered the most versatile corrosion resistant alloy available. This alloy is resistant to the formation of grain boundary precipitates in the weld heat-affected zone, thus making it suitable for most chemical process applications in an as welded condition. Alloy C-276 also has excellent resistance to pitting, stress-corrosion cracking and oxidizing atmospheres up to 1900°F. Alloy C-276 has exceptional resistance to a wide variety of chemical environments.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy b-3 b-2 pipe in China. If you're going to wholesale high quality hastelloy b-3 b-2 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy B-3 B-2 Tube

Hastelloy Alloy Products Description

This Nickel-Molybdenum alloy gives excellent resistance to hydrochloric acid at all concentrations and temperatures from ambient to high. It also withstands sulphuric, acetic, formic and phosphoric acids and other non-oxidizing media. B-3 also has excellent resistance to pitting corrosion and to stress-corrosion cracking. Hastelloy B-3 is not recommended in the presence of ferric or cupric salts. Like other nickel alloys, Hastelloy B-3 is ductile and can be formed and welded. It resists stress corrosion cracking in chloride-bearing solutions, and is able to withstand fluoride-bearing media and concentrated sulfuric acid, both of which result in damage to zirconium alloys.

Alloy B-2 is a solid solution strengthened, nickel-molybdenum alloy typically used in extreme reducing conditions. Alloy B-2 has significantly lower carbon, silicon and iron compared to the predecessor, alloy B (UNS N10001). Compared to alloy B, alloy B-2 is less susceptible to weld zone corrosion in the as-welded condition. Controlling other alloying elements such as iron and chromium resolved potential issues with forming and shaping. Stringent chemistry control in the production of alloy B-2 allows the alloy to be used in the welded condition, and it is less susceptible to stress corrosion cracking under many conditions. Care must be taken in selecting the right alloy for the desired application. Alloy B-2 should not be used at temperatures between 1000°F and 1600°F as the alloy forms secondary phases that could decrease the ductility

 

Chemical Composition Products Description
(Ni) Nickel Remainder
(Mo) Molybdenum 26.0 to 30.0
(Fe) Iron 2.00 max
(Cr) Chromium 1.00 max
(Co) Cobalt 1.00 max
(Mn) Manganese 1.00 max
(Si) Silicon 0.10 max
(P) Phosphorus 0.040 max
(S) Sulfur 0.030 max
(C) Carbon 0.02 max

Hot Tags: hastelloy b-3 b-2 pipe, China hastelloy b-3 b-2 pipe suppliers, alloy for marine applications, UNS N06455 N10629 Hastelloy Pipe, high temperature corrosion resistant alloy, nickel chromium molybdenum tungsten alloy, hastelloy ss pipe, alloy for petrochemical applications