G30 C4 Alloy Hastelloy hollow Tube
Dimensions: 1000mm x 2000mm, 1220mm x 2440mm, 1500mm x 3000mm, 2000mm x 2000mm, 2000mm x 4000mm
Thickness: 0.1mm to 100mm
Width: 10-2500mm
Length: 2m, 2.44m, 3m or as per requirement
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of g30 c4 alloy hastelloy hollow tube in China. If you're going to wholesale high quality g30 c4 alloy hastelloy hollow tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy Pipe Products Application
g30 c4 alloy hastelloy seamless tube video
Hastelloy G30 Tube Specifications
| Size | 15 NB to 150 NB IN |
|---|---|
| Type | Seamless / ERW / Welded / Fabricated / Hollow / LSAW Pipes |
| wall thickness | 035" –.095′, (special wall thicknesses available) |
| Schedule | SCH5, SCH10, SCH40, STD, SCH80, SCH160 |
| Finish | Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF |
| Form | Round, Square, Rectangular, Hydraulic, Straight or 'U' bent Tubes Etc |
| Length | Single Random, Double Random & Cut Length. |
| End | Plain End, Beveled End, Treaded. |
Product Specifications: Hastelloy C4 Tube
Specifications: ASTM / ASME
Sizes: 1/2" to 48" ID and OD (Welded Thickness: 1mm to 40mm)
Seamless Thickness: Sch10, Sch20, Sch30, Sch40, Sch60, Sch80
Types: Seamless, Welded (ERW), MAT, Polished, BA, Mirror Polished
Shapes: Tube, Pipe, Square, Rectangular
Hastelloy Material Specification
Hastelloy G-30 Tube Chemical Composition
| Element | Content (%) |
|---|---|
| Nickel, Ni | 43 |
| Chromium, Cr | 28.0-31.5 |
| Iron, Fe | 13-17 |
| Cobalt, Co | 5 |
| Molybdenum, Mo | 4-6 |
| Tungsten, W | 1.50 – 4 |
| Manganese, Mn | 1.50 |
| Copper, Cu | 1 – 2 .40 |
| Silicon, Si | 0.8 |
| Phosphorous, P | 0.040 |
| Carbon, C | 0.030 |
| Sulfur, S | 0.020 |
Hastelloy C4 Seamless Pipe Chemical Composition
| Chemical Composition | C | Mn | P | S | Si | Cr | Ni | Mo | Fe |
| N06455 | 0.015 | 1.00 | 0.04 | 0.03 | 0.08 | 14-18 | Balance | 14-17 | 3 |


Hastelloy G30 Tube is a corrosion resistant alloy with excellent corrosion resistance in oxidizing environments. Hastelloy G30 Tube has been successfully used in phosphoric acid heat exchanger tubes and other process components in the fertilizer industry. Both Hastelloy G30 Tubes contain high chromium and are the material of choice for strong oxidizing solutions and mixed pickling. We keep Hastelloy G30 Seamless Tubes and Hastelloy G30 Welded Tubes in stock. We are a well-known supplier and distributor of Hastelloy G30/ G35 Seamless Tubes. We have a team of experienced technical experts with extensive experience in Alloy G30/ G35 Seamless Tubes.
Hastelloy C4 alloy is an austenitic low carbon nickel-molybdenum-chromium alloy. The main difference from other alloys of similar chemical composition developed earlier is the low carbon, silicon, iron, tungsten content and the addition of stabilizing elements titanium. Such a chemical composition is more suitable for manufacturing corrosion-resistant equipment that requires welding, and also has good cold and hot plasticity. It shows good stability at 650-1040℃, improves the ability to resist intergranular corrosion, and can avoid edge line corrosion sensitivity and weld heat affected zone corrosion under appropriate manufacturing conditions.
Products Description
G30 C4 Alloy hollow Tube

Customer Case
customer visit


FAQ
Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: About the product price of g30 c4 alloy hastelloy tube?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Contact Us
Address
No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China
Phone
+86-15824687445
ss@gneesteel.com