Uns N06022 C2000 Hastelloy Tube
video

Uns N06022 C2000 Hastelloy Tube

C22 (N06022) Hastelloy alloy, material number 2.6402, is a nickel-based high-temperature alloy composed of nickel, molybdenum, cobalt, tungsten and other elements, with a nickel content of approximately 60%.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n06022 c2000 hastelloy tube in China. If you're going to wholesale high quality uns n06022 c2000 hastelloy tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy Pipe Products Application

uns n06022 c2000 Hastelloy ss Tube video

Pharmaceutical industries use alloy C-22 fittings and tubing to avoid contamination caused by corrosion related failures

Cellophane manufacturing

Chlorination systems

Pesticide production

Incineration scrubber systems

Chemical process industry in equipment like flue gas scrubbers, chlorination systems, sulfur dioxide scrubbers, pulp and paper bleach plants, pickling systems, and nuclear fuel reprocessing

Waste water processing

Hastelloy Material Specification

 

C22 – UNS N06022
Element Simbol Maximum
Carbon C 0,015
Manganese Mn 0,50
Tungsten W 2,5-3,5
Sulfur S 0,020
Silicon Si 0,08
Nickel Ni 56,0
Chrome Cr 20,0-22,5
Molybdenum Mo 12,5-14,5
Cobalt Co 2,5
Iron Fe 2,0-6,0
Phosphorus P 0,02
Vanadium V 0,35

uns n06022 c2000 Hastelloy alloy Tube suppliersuns n06022 c2000 material Tube price

C22 (N06022) Hastelloy alloy, material number 2.6402, is a nickel-based high-temperature alloy composed of nickel, molybdenum, cobalt, tungsten and other elements, with a nickel content of approximately 60%. It is a versatile nickel-chromium-molybdenum-tungsten alloy with better overall corrosion resistance than other existing nickel-chromium-molybdenum alloys, including Hastelloy C-276, Alloy C4, and Alloy 625. Hastelloy C22 alloy has good resistance to pitting corrosion, crevice corrosion and stress corrosion.
Hastelloy C-2000, named UNS N06200, is a nickel-based alloy composed of nickel, molybdenum, chromium and other elements, with a nickel content of about 55%. Adding a certain amount of copper to sulfuric acid, hydrofluoric acid, and dilute hydrochloric acid can improve its temperature performance. The high chromium content provides maximum resistance to oxidizing chemicals and process streams contaminated by iron ions and dissolved oxygen. The alloy has excellent resistance to chloride corrosion and corrosion.

Customer Case

customer visit

uns n06022 c2000 Hastelloy steel Tube factory

uns n06022 c2000 Hastelloy stainless steel Tube price

FAQ

 

 

 

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.

Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.

Q: About the product price of uns n06022 c2000 Hastelloy Tube?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: uns n06022 c2000 hastelloy tube, China uns n06022 c2000 hastelloy tube suppliers, alloy for annealing, alloy for drawing, alloy for batteries, alloy for petrochemical applications, alloy for nuclear power plants, alloy for scrubbers