C-276 Hastelloy Metal Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of c-276 hastelloy metal pipe in China. If you're going to wholesale high quality c-276 hastelloy metal pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
C-276 Hastelloy Alloy Pipe Equivalent grade
C-276 Hastelloy Metal Pipe video
GNEE STEEL COMPANY
Our company is engaged in the production and trade of various alloy C-276 Hastelloy Metal Pipe, high-performance, high-precision special-shaped steel pipes and seamless pipes. We have established business relationships with customers in more than 20 countries and regions. Details such as payment method, delivery time and minimum quantity can be negotiated based on the order.
UNS Number N10276
W.Nr. 2.4819
Other common names: Alloy C276, Hastelloy C, Inconel® C-276
ASTM B574, B564, B575, B619, B626, B622
ASME SB574, SB564, SB575, SB619, SB626, SB622
C-276 Hastelloy Pipe chemical composition
| Element | Min % | Max % |
|---|---|---|
| Cr | 20.50 | 23.00 |
| Mo | 8.00 | 10.00 |
| Fe | 17.00 | 20.00 |
| W | 0.20 | 1.00 |
| C | 0.05 | 0.15 |
| Si | – | 1.00 |
| Co | 0.50 | 2.50 |
| Mn | – | 1.00 |
| P | – | 0.04 |
| S | – | 0.03 |
| B | – | 0.01 |
| Ni | bal |
C-276 Hastelloy Metal Pipe chemical composition


Hastelloy X Nickel-based superalloy Hastelloy X is a nickel-chromium-molybdenum alloy with added cobalt and tungsten. Hastelloy X alloy has excellent oxidation resistance at high temperatures up to 1200°C and can also be used in neutral and reducing atmospheres.
Hastelloy B-3 is a nickel-molybdenum alloy with excellent resistance to hydrochloric acid at all concentrations and temperatures. It is also resistant to sulfuric acid, acetic acid, formic acid and phosphoric acid as well as other non-oxidizing media.
Hastelloy C-276 is an alloy with extremely low silicon-carbon content and is considered a universal corrosion-resistant alloy. Mainly resistant to wet chlorine, various oxidizing chlorides, chloride salt solutions, sulfuric acid and oxidizing salts, and has good corrosion resistance in low and medium temperature hydrochloric acid.
Specifications |
|
|---|---|
| Form |
Standard |
|
UNS |
UNS N10276 |
|
Bar |
ASTM B574 Din 17752 |
|
Wire |
|
|
Sheet |
ASTM B575 Din 17750 |
|
Plate |
ASTM B575 Din 17750 |
|
Fitting |
ASTM B366 |
|
Forging |
ASTM B564 |
|
Tube |
ASTM B619 ASTM B622 ASTM B626 Din 17751 |
|
Pipe |
ASTM B619 ASTM B622 ASTM B626 Din 17751 |
|
Weld Wire |
A5.14 ERNiCrMo-4 |
|
Weld Electrode |
A5.11 ENiCrMo-4 |
|
Din. |
2.4819 All Forms |
The mechanical properties of HASTELLOY(r) C276 are displayed in the following table.
| Properties | Metric | Imperial |
|---|---|---|
| Tensile strength (thickness 4.80-25.4 mm, 538°C/thickness 0.189-1.00 in, 1000°F) | 601.2 MPa | 87200 psi |
| Yield strength (0.2% offset, thickness 2.40 mm, 427°C/thickness 0.0945 in, 801°F) | 204.8 MPa | 29700 psi |
| Elastic modulus (RT) | 205 GPa | 29700 ksi |
| Elongation at break (in 50.8 mm, thickness 1.60-4.70 mm, 204°C/thickness 0.0630-0.185 in, 399°F) | 56% | 56% |
| Hardness, Rockwell B (plate) | 87 | 87 |
GNEE company team
GNEE company team

GNEE C-276 Hastelloy Metal Pipe certificate
GNEE C-276 Hastelloy Pipe certificate

GNEE Group participated in the NECC exhibition
GNEE Group participated in the NECC exhibition

C-276 Hastelloy Steel Pipe packaging
C-276 Hastelloy Round Alloy Pipe packing

C-276 Hastelloy Metal SS Pipe size & material
C-276 Hastelloy Pipe


Customer Case
GNEE customer visit


FAQ
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.
Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.
Q: About the product price of C-276 Hastelloy Metal Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Contact Us
One-stop service, making choices easier.
![]()
Phone
+8615824687445
+86-372-5055135
![]()
ss@gneesteel.com
![]()
Address
No.4-1114, Beichen Building, Beicang Town, Beichen District, Tianjin, China
Hot Tags: C-276 Hastelloy Metal Pipe, China C-276 Hastelloy Metal Pipe suppliers, alloy for tempering, hastelloy alloy, B C4 Piping, nickel chromium molybdenum tungsten alloy, alloy for drawing, alloy for valves
You Might Also Like
Send Inquiry