C-276 C22 C4 Hastelloy Heat treated Pipe
video

C-276 C22 C4 Hastelloy Heat treated Pipe

Hastelloy C4 Tube Specifications
Specifications: ASTM B622, B619, B626 / ASME SB622, SB619, SB626
Standards: ASTM, ASME and API
Size Range: 15" NB – 150" NB
OD: 1.250" – 6.000" (30-150 mm)
Wall Thickness Range: 0.095" – 1.000" (0.2.5-25 mm)
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of c-276 c22 c4 hastelloy heat treated pipe in China. If you're going to wholesale high quality c-276 c22 c4 hastelloy heat treated pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

C-276 C22 C4 Hastelloy Pipe Equivalent grade

C-276 C22 C4 Heat treated Pipe video

GNEE STEEL GROUP supplies Hastelloy C-276 C22 C4 Alloy Pipe for you

 

GNEE STEEL GROUP supplies Hastelloy C-276 Alloy Pipe

UNS Number N10276

W.Nr. 2.4819

Other common names: Alloy C276, Hastelloy C, Inconel® C-276

ASTM B574, B564, B575, B619, B626, B622

ASME SB574, SB564, SB575, SB619, SB626, SB622

What forms of Hastelloy C276 does GNEE STEEL offer?
bar
sheet
plate
Pipes and Tubes – Welded and Seamless
Accessories
Elbows, tees, short pipe ends, return pipes, pipe caps, crosses, reducers, pipe joints. ETC.
Welding wire (AWS classification: ERNiCrMo-4 and ENiCrMo-4)

Specifications

Form

Standard

UNS

UNS N10276

Bar

ASTM B574 Din 17752

Wire

 

Sheet

ASTM B575 Din 17750

Plate

ASTM B575 Din 17750

Fitting

ASTM B366

Forging

ASTM B564

Tube

ASTM B619 ASTM B622 ASTM B626 Din 17751

Pipe

ASTM B619 ASTM B622 ASTM B626 Din 17751

Weld Wire

A5.14 ERNiCrMo-4

Weld Electrode

A5.11 ENiCrMo-4

Din.

2.4819 All Forms

 

GNEE STEEL GROUP supplies Hastelloy C22 Alloy Pipe

UNS Number N06022

W.Nr. 2.4602

Other common names: Alloy C22

ASTM B574, B564, B575, B619, B626, B622

ASME SB574, SB564, SB575, SB619, SB626, SB622

What forms of Hastelloy C22 does GNEE STEEL offer?
bar
sheet
plate
Pipes and Tubes – Welded and Seamless
Accessories
Elbows, tees, short pipe ends, return pipes, pipe caps, crosses, reducers, pipe joints. ETC.
Welding wire (AWS classification: ERNiCrMo-4 and ENiCrMo-4)

GNEE STEEL GROUP supplies Hastelloy C4 Alloy Pipe

W.NR 2.4610
UNS N06455
AWS 052

Hastelloy C4/C22/C276 Pipe Specifications

Pipe Specification : ASTM B622, B619 / ASME SB622, SB619
Dimension Standard : ANSI B36.19M, ANSI B36.10
Hastelloy C276 Pipe Size : 1/4" sch 10 to 16" sch 80
Hastelloy C276 Tube Size : OD 1/16"~4", Wall: 0.010"~0.250", Length: 17'/24' FT R/L
Outside Diameter : 6.35 mm OD upto 254 mm OD in 0.6 TO 20 mm thickness
Type : Seamless / ERW / Welded / Fabricated Pipes
Form : Round, Square, Rectangular, Oval, Hydraulic Etc
Length : Single Random, Double Random & Required Length
End : Plain End, Beveled End, Treaded
End Protection : Plastic Caps

C-276 C22 C4 Hastelloy Pipe chemical composition

Hastelloy C276 Alloy Pipe chemical composition

Ni Mo Cr Fe W Co Mn C V P S Si

Remainder

15.0-17.0

14.5-16.5

4.0-7.0

3.0-4.5

2.5 max

1.0 max

.01 max

.35 max

.04 max

.03 max

.08 max

Hastelloy C22 Alloy Pipe chemical composition

C Cr Co Fe Mn Mo Ni P Si S W V

.010 max

20-22.5

2.5 max

2.0-6.0

.50 max

12.5-14.5

Balance

.02 max

.08 max

.02 max

2.5-3.5

.35 max

Hastelloy C4 Alloy Pipe Chemical Composition

The chemical composition of Hastelloy C-4 is indicated in the table below:

Element Min % Max %
Cr 14.00 18.00
Mo 14.00 17.00
Fe – 3.00
C – 0.015
Si – 0.08
Co – 2.00
Mn – 1.00
P – 0.04
S – 0.03
Ti – 0.70
Ni Bal

C-276 C22 C4 hastelloy pipe

C-276 C22 C4 hastelloy tubing suppliersC-276 C22 C4 hastelloy seamless pipe dealer

Hastelloy C-276 alloy is one of the few materials that can be used in hot concentrated H2SO4 solutions. It is mainly resistant to wet chlorine, various oxidizing chlorides, chloride salt solutions, H2SO4 and oxidizing salts, and is resistant to both low and medium temperature HCl. Has very good corrosion resistance. Therefore, in the past thirty years, it has been widely used in harsh corrosive environments, such as chemical industry, petrochemical industry, flue gas desulfurization, pulp and paper making, environmental protection and other industrial fields.
Hastelloy C22 alloy is a versatile nickel-chromium-molybdenum-tungsten alloy that has better overall corrosion resistance than other existing nickel-chromium-molybdenum alloys, including Hastelloy C276, C4 alloy and 625 alloy. Hastelloy C22 alloy has good resistance to pitting corrosion, crevice corrosion and stress corrosion cracking.
Hastelloy C4 alloy is an austenitic low carbon nickel-molybdenum-chromium alloy. The main difference from other alloys of similar chemical composition developed earlier is the low carbon, silicon, iron, tungsten content and the addition of stabilizing elements titanium.

GNEE Group Product Packaging

C-276 C22 C4 alloy Heat treated Pipe

C-276 C22 C4 Hastelloy Pipe

C-276 C22 C4 Hastelloy Pipe material & size

C-276 C22 C4 Hastelloy Pipe material & size

C-276 C22 C4 Hastelloy Pipe

C-276 C22 C4 Hastelloy Pipe

 

Customer Case

customer visit

C-276 C22 C4 Hastelloy Pipe

 

FAQ

Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.

Q: What are your payment terms?
A: Payment <=1000USD, 50% in advance. Payment >=1000USD, 30% T/T in advance, balance before shipment. or negotiable

Q: About the product price of C-276 C22 C4 hastelloy pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: C-276 C22 C4 Hastelloy Heat treated Pipe, China C-276 C22 C4 Hastelloy Heat treated Pipe suppliers, alloy for welding, alloy for heat treatment, hastelloy alloy piping, seamless pipe alloy, alloy for batteries, alloy for desalination plants