Duplex 2207
video

Duplex 2207

UNS S32750, F53 ASTM A 240, A790, A815, A182, A 276, A 476, A789 EN 1.4410
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of duplex 2207 in China. If you're going to wholesale high quality duplex 2207 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

 
GNEE Duplex 2207 Description
 

Duplex 2207 video

Stainless steel Super Duplex 2507 is designed to handle highly corrosive conditions and situations were high strength is required. High molybdenum, chromium and nitrogen content in Super Duplex 2507 help the material withstand pitting and crevice corrosion. The material is also resistant to chloride stress corrosion cracking, to erosion corrosion, to corrosion fatigue, to general corrosion in acids. This alloy has good weldability and very high mechanical strength.

 

The following sections will discuss in detail about stainless steel grade Super Duplex 2507.

STANDARD WERKSTOFF NR. UNS JIS AFNOR BS GOST EN
Super Duplex 2207 1.4501 S32750 / S32760 SUS 329J3L Z3 CrNi 22.05 AZ – – X2CrNiMoN 22.5.3

 

 

GNEE STEEL offers Super Duplex 2507 form
sheet
plate
bar
Pipes and Tubes (Welded and Seamless)
Accessories
Elbows, tees, short pipe ends, return pipes, pipe caps, crosses, reducers, pipe joints, etc.
Welding wire AWS ER2594, E2594-16, E2553T-1 

GNEE STEEL Duplex 2207 Chemical Composition
 

 

The chemical composition of stainless steel grade Super Duplex 2507 is outlined in the following table.

Element Content (%)
Chromium, Cr 24 – 26
Nickel, Ni 6 – 8
Molybdenum, Mo 3 – 5
Manganese, Mn 1.20 max
Silicon, Si 0.80 max
Copper, Cu 0.50 max
Nitrogen, N 0.24 – 0.32
Phosphorous, P 0.035 max
Carbon, C 0.030 max
Sulfur, S 0.020 max
Iron, Fe Balance

 

GNEE STEEL Duplex 2207 Application
 

Desalination Equipment

Chemical process pressure vessels, piping and heat exchangers

Marine Applications

Flue Gas Scrubbing Equipment

Pulp & Paper Mill Equipment

Offshore Oil production/technology

Oil and gas industry equipment

 

GNEE Duplex 2207 Feature
 

 

High resistance to chloride stress corrosion cracking

High Strength

Superior resistance to chloride pitting and crevice corrosion

Good general corrosion resistance

Suggested for applications up to 600° F

Low rate of thermal expansion

Combination of properties given by austenitic and ferritic structure

Good weldability and workability

GNEE Duplex 2207 Reference Standards
 

Plate, sheet and coil:

ASTM A240, EN 10028-7, EN 10088-2, EN 10088-4, Norsok M-630 MDS D45

Bar and forging:

ASTM A276, ASTM A479, ASTM A182, EN 10088-3, Norsok M-630 MDS D44/D47

Other products:

As per applicable ASTM and/or EN standards and Norsok M-630 MDS

 

GNEE Duplex 2207 ASTM Specifications
 

 

Pipe Smls Pipe Welded Tube Smls Tube Welded Sheet/Plate Bar Flanges & Fittings

A790

A790

A789

A789

A240

A276

A182

 

GNEE Duplex 2207 form Size
 


Pipe Stock Size

OD MM ID MM WEIGHT KG/M
45 28 8,07
50 25 11,98
71 45 19,43
90 63 26,87
106 56 51,52
112 63 54,71
112 80 40,07
118 80 48,71
125 90 49,15
132 106 41,53
132 90 61,41
140 100 62,60
150 106 73,33
160 112 84,88
170 128 83,50
190 132 121,29
212 170 107,62
236 150 213,51
250 200 150,80

 

Sheet stock Size

MEASUREMENTS KG/PLATE
0,5 x 1500 x 3000 mm 18
1 x 1000 x 2000 mm 16
1 x 1500 x 3000 mm 36
1,5 x 1500 x 3000 mm 54
2 x 1000 x 2000 mm 32
2 x 1500 x 3000 mm 72
3 x 1500 x 3000 mm 108
3 x 1500 x 6000 mm 216
3 x 2000 x 6000 mm 288
4 x 1500 x 3000 mm 144
4 x 1500 x 6000 mm 288
4 x 2000 x 6000 mm 384
5 x 1500 x 3000 mm 180
5 x 1500 x 6000 mm 360
5 x 2000 x 6000 mm 480
6 x 1500 x 3000 mm 216
6 x 1500 x 6000 mm 432
6 x 2000 x 6000 mm 576
8 x 1500 x 3000 mm 297
8 x 1500 x 6000 mm 594
8 x 2000 x 6000 mm 791
10 x 1500 x 3000 mm 371
10 x 1500 x 6000 mm 742
10 x 2000 x 6000 mm 989

 

MEASUREMENTS KG/PLATE
12 x 1500 x 3000 mm 445
12 x 1500 x 6000 mm 890
12 x 2000 x 6000 mm 1187
15 x 1500 x 3000 mm 557
15 x 1500 x 6000 mm 1113
15 x 2000 x 6000 mm 1484
20 x 1500 x 3000 mm 742
20 x 1500 x 6000 mm 1484
20 x 2000 x 6000 mm 1978
25 x 1500 x 3000 mm 927
25 x 1500 x 6000 mm 1854
25 x 2000 x 6000 mm 2472
30 x 1500 x 3000 mm 1113
30 x 1500 x 6000 mm 2225
30 x 2000 x 6000 mm 2967
35 x 2000 x 6000 mm 3360
40 x 1500 x 3000 mm 1484
40 x 1500 x 6000 mm 2967
40 x 2000 x 6000 mm 3956
45 x 2000 x 4000 mm 2880
50 x 1500 x 3000 mm 1854
50 x 1500 x 6000 mm 3708
50 x 2000 x 6000 mm 4944
60 x 1500 x 3000 mm  
80 x 1500 x 3000 mm  

 

Coil Stock Size

1300 MM 1500 MM 2000 MM
0,4 mm 1,5 mm 3 mm
0,5 mm 2 mm 4 mm
1 mm 3 mm 5 mm
  4 mm 6 mm
  5 mm  
  6 mm  

 

Round Bar Stock Size

DIA KG/M
6 mm 0.3
8 mm 0.4
10 mm 0.6
12 mm 1.
16 mm 1.7
20 mm 2.6
25 mm 4.
30 mm 5.6
35 mm 7.7
40 mm 10.1
45 mm 12.7
50 mm 15.7
60 mm 22.6
70 mm 30.8
80 mm 40.2
90 mm 50.9
100 mm 62.9
110 mm 76.1
120 mm 90.5
125 mm 98.7
130 mm 106.
140 mm 123.
150 mm 141
160 mm 161
170 mm 182

 

DIA KG/M
180 mm 204
185 mm 215
190 mm 228
200 mm 251
202 mm 258
210 mm 278
220 mm 304
225 mm 319
230 mm 333
240 mm 362
250 mm 385
265 mm 438
275 mm 476
280 mm 493
300 mm 566
310 mm 612
320 mm 645
330 mm 686
350 mm 780
355,6 mm 805
365 mm 840
375 mm 880
380 mm 910
400 mm 995
410 mm 1058

 

Our Company
 

 

duplex 2207 company

1 -

Customer Visit
 

duplex 2207 customer visit

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide

 

FAQ
 

 

Q: What is your terms of payment ?

A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable.

Q: Can you provide sample ?

A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Q:Can you send samples?

A:Of course, we can send samples to all parts of the world, our samples are free, but customers need to bear the courier costs.

Q: About the product price of Duplex 2207?

A: Due to cyclical changes in raw material prices, prices vary in different periods.

 

Hot Tags: duplex 2207, China duplex 2207 suppliers, duplex stainless steel stock, duplex stainless steel optimization, duplex stainless steel comparison, duplex stainless steel installation, duplex stainless steel distributor, duplex stainless steel manufacturing

Send Inquiry

whatsapp

Phone

E-mail

Inquiry