Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 904l stainless steel bar in China. If you're going to wholesale high quality 904l stainless steel bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
904l Stainless Steel bar Description & Equivalent grade
904l Stainless Steel video
GNEE STEEL GROUP supplies 904l Stainless Steel bar for you
Grade 904L stainless steel bar is a non-stabilized austenitic stainless steel with low carbon content. This high-alloy stainless steel has copper added to improve its resistance to strong reducing acids such as sulfuric acid. The steel is also resistant to stress corrosion cracking and crevice corrosion. Grade 904L rod is non-magnetic and offers excellent formability, toughness and weldability.
Grade 904L rod contains significant amounts of expensive ingredients such as molybdenum and nickel. Today, most applications using grade 904L rod have been replaced by the low-cost duplex stainless steel 2205. The following sections describe the characteristics of flat-rolled products in ASTM B625. Specifications may vary for other products such as rod, tube and pipe.
Specification of 904L Stainless Steel Round Bar
| 904L SS Round bar size | Diameter: 3-~800mm |
|---|---|
| Alloy 904L Hex Bar size | 2-100mm A/F |
| 904L Steel Flat bar size | Thickness: 2 -100mm |
| Width: 10 to 500mm | |
| ASTM A276 UNS N08904 Square bar size | 4 to 100mm |
| 904L Grade Stainless Steel Angle bar size (in mm) | 3*20*20~12*100*100 |
| 904L Stainless Steel Section | 3.0 to 12.0mm thickness |
| N08904 Stainless Steel Channel Bar (in mm) | 80 x 40 to 150 x 75 section; 5.0 to 6.0 thickness |
| Stainless Steel 1.4539 Hollow Bar (in mm) | 32 OD x 16 ID to 250 OD x 200 ID) |
| SS 904L Billet Size | 1/2" to 495mm Diameter |
| Stainless Steel 904L Rectangles Size | 33 x 30mm to 295 x 1066mm |
| Alloy 904L Round Bar Finish | Cold (bright) drawn, centreless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centreless Ground & Black |
| 904L Steel Round Bar Surface | Bright, Hot Rolled Pickled, Cold Drawn, Sand Blasting Finished, Polished, Hairline |
| 904L Stainless Steel Round Bar Condition | Hardened & tempered, annealed |
| Our 904L Steel Round bar conforms to NACE MR0175/ISO 15156 | |
904l Stainless Steel bar chemical composition
904l Stainless Steel bar chemical composition
| Element | Min | Max |
|---|---|---|
| C | - | 0.02 |
| Mn | - | 2 |
| Ni | 23 | 28 |
| Cr | 19 | 23 |
| S | - | 0.03 |
| Mo | 4 | 5 |
| N | - | 0.1 |
| Cu | 1 | 2 |
| P | - | 0.03 |
| Si | - | 1 |
904l Stainless Steel Parameter & chemical composition



904l Stainless Steel bar Application
Our stainless steel 904L rods are used in a wide range of applications and various industries. Here are some of them:
Petrochemical industry
oil and gas industry
chemical industry
Power plant industry
energy industry
Pharmaceutical industry
Pulp and paper industry
food processing industry
aerospace industry
Refining industry
904l Stainless Steel bar Feature
Cold rolled products have good appearance and gloss
Good high temperature strength
Good work hardening (weak magnetism after processing)
nonmagnetic solution
Suitable for building, construction and other applications
DIMENSIONS OF STAINESS STEEL 904L ROUND BAR
Stainess Steel 904L Bar Weight Chart
![]()
| Size | Kgs / Foot | Kgs / Mtr | Size | Kgs / Foot | Kgs / Mtr | Size | Kgs / Foot | Kgs / Mtr |
|---|---|---|---|---|---|---|---|---|
| 3mm | 0.017 | 0.055 | 20mm | 0.753 | 2.470 | 3" | 10.900 | 35.762 |
| 1/8" | 0.019 | 0.062 | 22mm | 0.908 | 2.979 | 3-1/4" | 12.800 | 41.996 |
| 5/32" | 0.029 | 0.095 | 7/8" | 0.926 | 3.038 | 3-1/2" | 14.850 | 48.772 |
| 4mm | 0.030 | 0.098 | 24mm | 1.080 | 3.543 | 3-3/4" | 17.001 | 55.780 |
| 3/16" | 0.043 | 0.141 | 25mm | 1.180 | 3.871 | 4" | 19.306 | 63.340 |
| 5mm | 0.047 | 0.154 | 1" | 1.210 | 3.970 | 4-1/4" | 21.908 | 72.249 |
| 7/32" | 0.058 | 0.190 | 26mm | 1.271 | 4.170 | 4-1/2" | 24.4487 | 80.340 |
| 6mm | 0.068 | 0.223 | 27mm | 1.368 | 4.490 | 4-3/4" | 27.366 | 90.249 |
| 1/4" | 0.076 | 0.249 | 1-1/8" | 1.534 | 5.033 | 5" | 30.461 | 99.940 |
| 7mm | 0.091 | 0.298 | 30mm | 1.691 | 5.548 | 5-1/2" | 36.690 | 121.000 |
| 5/16" | 0.118 | 0.387 | 1-1/4" | 1.924 | 6.349 | 6" | 43.860 | 143.900 |
| 8mm | 0.120 | 0.398 | 32mm | 1.894 | 6.314 | 6-1/2" | 51.093 | 167.630 |
| 9mm | 0.152 | 0.498 | 1-3/8" | 2.303 | 7.550 | 7" | 59.432 | 196.000 |
| 3/8" | 0.170 | 0.557 | 35mm | 2.390 | 7.553 | 7-1/2" | 68.226 | 225.000 |
| 10mm | 0.189 | 0.620 | 36mm | 2.438 | 7.999 | 8" | 77.586 | 254.55 |
| 11mm | 0.228 | 0.748 | 38mm | 2.792 | 8.903 | 10" | 121.048 | 397.140 |
| 7/16" | 0.232 | 0.761 | 1-1/2" | 2.715 | 8.951 | |||
| 12mm | 0.271 | 0.889 | 40mm | 3.009 | 9.872 | |||
| 1/2" | 0.303 | 0.994 | 1-5/8" | 3.200 | 10.449 | |||
| 13mm | 0.318 | 1.043 | 1-3/4" | 3.712 | 12.179 | |||
| 14mm | 0.368 | 1.207 | 45mm | 3.807 | 12.555 | |||
| 9/16" | 0.383 | 1.256 | 1-7/8" | 4.260 | 13.977 | |||
| 15mm | 0.424 | 1.391 | 48mm | 4.330 | 14.205 | |||
| 5/8" | 0.473 | 1.551 | 50mm | 4.698 | 15.414 | |||
| 16mm | 0.481 | 1.578 | 2" | 4.848 | 15.906 | |||
| 17mm | 0.543 | 1.791 | 2-1/8" | 5.475 | 17.963 | |||
| 11/16" | 0.573 | 1.880 | 2-1/4" | 6.135 | 20.128 | |||
| 18mm | 0.610 | 2.001 | 60mm | 6.768 | 22.205 | |||
| 3/4" | 0.682 | 2.237 | 2-3/8" | 6.838 | 22.435 | |||
| 2-1/2" | 7.576 | 24.856 | ||||||
| 2-5/8" | 8.354 | 27.409 | ||||||
| 2-3/4" | 9.169 | 30.083 |
GNEE company team
GNEE company team

904l Stainless Steel bar material
904l Stainless Steel material


Stainless steel not only has corrosion resistance, but also has advantages such as heat resistance, processability, strength, and appearance. GNEE Steel utilizes the properties of stainless steel to improve quality through various surface treatments. Baoxin Steel provides different types of stainless steel surface treatment processes, such as BA, 2B, 2D, 2K, 4K, 6K, 8K, NO.4, HL, SB, embossing, etc.
List of 904L Stainless Steel Round Bar Types
| Stainless Steel 904L Round Bar | ASTM A276 UNS N08904 Flat Bar |
| 904L SS Bar | 904L Steel Flat Bar Black |
| Alloy 904L Rounds | 904L Grade Stainless Steel Flat Bar Bright |
| 904L Steel Bright Bar | 904L Stainless Steel Flat Bar Polished |
| ASTM A276 UNS N08904 Rods | 904L SS Flat Bar Cold Drawn |
| Alloy 904L Square Bar Cold Drawn | 904L SS Bright Bar material |
| 904L Grade Stainless Steel Rod | Stainless Steel 904L Flat Bar Annealed |
| 904L Stainless Steel Round Bars | 904L SS Flat Bar stock |
| N08904 Stainless Steel Hex Bar | Alloy 904L Threaded Bar |
| 904L SS Square Bar Polished | Stainless Steel 904L Bright Bar Hot Rolled |
| SS 904L Hex Bar Bright | ASTM A276 UNS N08904 Hollow Bar |
| Stainless Steel 1.4539 Rectangular Bar Annealed | 904L Steel Polished Hex Bar |
| Stainless Steel 904L Hex Bar Polished | 904L Grade Stainless Steel Hexagonal Bar |
| SS 904L Rectangular Bar | N08904 Stainless Steel Threaded Bar Black |
| 904L Steel Hex Bar Annealed | N08904 Stainless Steel Cold Drawn Round Bar |
| 904L Grade Stainless Steel Forged Bar | Stainless Steel 1.4539 Polished Bar |
GNEE Group participated in the NECC exhibition
GNEE Group participated in the NECC exhibition

GNEE product certificate
GNEE product certificate

904l Stainless Steel bar Packing & Delivery
904l Stainless Steel Packing & Delivery

Customer Visit
Customer Visit

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide
FAQ
Q:What is your delivery time ?
A: Our delivery time is about one week, timing according to the number of customers.
Q: How long is your delivery time?
A: It is according to quantity. Generally it is 30 days.
Q:What are the shipping ports?
A:Under normal circumstances, we ship from Tianjin port, you can choose other ports according to your needs.
Q:Can you send samples?
A:Of course, we can send samples to all parts of the world, our samples are free, but customers need to bear the courier costs.
Contact Us
Contact Us
Hot Tags: 904l Stainless Steel bar, China 904l Stainless Steel bar suppliers, duplex stainless steel product, duplex stainless steel weight, duplex stainless steel fitting, duplex stainless steel durability, duplex stainless steel certification, duplex stainless steel refund
Next
Duplex 2207You Might Also Like
Send Inquiry