1.4835 stainless steel square tube
video

1.4835 stainless steel square tube

• Side Length: 4×4-300×300mm (Minimum - Maximum) • Wall Thickness: 0.25-10.0mm (Minimum – Maximum) • Length: 18000mm (Maximum) • *Customized size needs to be confirmed with us
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4835 stainless steel square tube in China. If you're going to wholesale high quality 1.4835 stainless steel square tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

1.4835 stainless steel square tube Description
 

1.4835 Stainless Steel video

253MA s30815 1.4835 Stainless steel is a lean austenitic heat resistant alloy with high strength and outstanding oxidation resistance. 253 MA maintains its heat resistant properties by advanced control of micro alloy additions. The use of rare earth metals in combination with silicon gives superior oxidation resistance up to 2000°F. Nitrogen, carbon and a dispersion of rare earth and alkali metal oxides combine to provide creep rupture strength comparable to the nickel base alloys. A wide variety of components requiring high strength at elevated temperatures such as heat exchangers, kilns, stack dampers and oven components are common applications for 253 MA.

 

Stainless steel 253 MA is readily fabricated by standard commercial procedures. In comparison to carbon steel, stainless steels are tougher and tend to work harden rapidly. However, with positive feeds and slow speeds combined with abundant cutting fluid this alloys tendency to work harden may be minimized. 253MA contains fairly low nickel content, which gives it some advantage in reducing sulphide atmospheres when compared to high nickel alloys and to Grade 310. The inclusion of high silicon, nitrogen and cerium contents gives the steel good oxide stability, high elevated temperature strength and excellent resistance to sigma phase precipitation.

 

• American Standard: ASTM A312, ASTM A358, ASTM A249, ASTM A269, ASTM A554, ASTM A790

• European Standard: DIN 17457

• Japanese Standard: JIS G3459

• GB Standard: GB/T12770-2002, GB/T12771-2008

1.4835 stainless steel square tube Chemical Composition
 

 

Grade DIN 1.4835
min max
C 0.05 0.10
Mn 0.80
Si 1.40 2.00
P 0.04
S 1.40 2.00
Cr 20.0 22.0
Ce 0.03 0.08
Ni 10.0 12.0
N 0.14 0.20
Fe Balance Balance

 

1.4835 stainless steel square tube1.4835 stainless steel square tube1.4835 stainless steel square tube

1.4835 stainless steel square tube Application
 

 

chemical industry
Thermal power plants and nuclear power plants
Fertilizer factory
aerospace
Food and dairy plants
paper industry
oil and gas exploration
desalination plant
pharmaceutical factory

 

1.4835 stainless steel square tube Feature
 

 

Excellent oxidation & aqueous resistance

Resistance to air at temperatures up to 1150°C.

High creep-rupture strength

Good formability and weldability

 

1.4835 stainless steel square tube Size
 
 
Side Width Wall Thickness Side Width Wall Thickness Side Width Wall Thickness
12.7 x 12.7 0.4 22 x 22 0.6 38 x 38 0.9
12.7 x 12.7 0.5 22 x 22 0.7 38 x 38 1.0
12.7 x 12.7 0.6 22 x 22 0.8 38 x 38 1.5
12.7 x 12.7 0.7 22 x 22 0.9 38 x 38 2.0
12.7 x 12.7 0.8 22 x 22 1.0 40 x 40 0.6
16 x 16 0.4 22 x 22 1.5 40 x 40 0.7
16 x 16 0.5 25 x 25 0.5 40 x 40 0.8
16 x 16 0.6 25 x 25 0.6 40 x 40 0.9
16 x 16 0.7 25 x 25 0.7 40 x 40 1.0
16 x 16 0.8 25 x 25 0.8 40 x 40 1.5
16 x 16 0.9 25 x 25 0.9 40 x 40 2.0
16 x 16 1.0 25 x 25 1.0 50 x 50 0.8
19 x 19 0.4 25 x 25 1.5 50 x 50 0.9
19 x 19 0.5 30 x 30 0.6 50 x 50 1.0
19 x 19 0.6 30 x 30 0.7 50 x 50 1.5
19 x 19 0.7 30 x 30 0.8 50 x 50 2.0
19 x 19 0.8 30 x 30 0.9 60 x 60 1.0
19 x 19 0.9 30 x 30 1.0 60 x 60 1.5
19 x 19 1.0 30 x 30 1.5 60 x 60 2.0
19 x 19 1.5 38 x 38 0.6 80 x 80 1.0
22 x 22 0.4 38 x 38 0.7 80 x 80 1.5
22 x 22 0.5 38 x 38 0.8 80 x 80 2.0
* Customized size needs to be confirmed with us

 

Customer Visit
 

 

1.4835 Stainless Steel

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide

FAQ
 

Q:About product prices?

A:Prices vary from period to period due to cyclical changes in the price of raw materials.

Q: Are you a factory or trading company?

A: We are professional manufacturer, and our company also is a very professional a trade company for steel products.We can provide a wide range of steel products.

Q:What do your factory do regarding quality control?

A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.

Q:Can you send samples?

A:Of course, we can send samples to all parts of the world, our samples are free, but customers need to bear the courier costs.

 

contact us
 

contact us

contact us

Hot Tags: 1.4835 stainless steel square tube, China 1.4835 stainless steel square tube suppliers, Super Duplex 2507, Duplex Stainless Steel, duplex 2207 stainless steel, Super Duplex 2507, , duplex 2207 stainless steel

Send Inquiry

whatsapp

Phone

E-mail

Inquiry