Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of duplex 1.4462 round bar in China. If you're going to wholesale high quality duplex 1.4462 round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Duplex 1.4462 round bar Description
Duplex 1.4462 VIDEO
Duplex 2205 is a stainless steel alloy known for its high strength, weldability, and corrosion resistance. Duplex 2205 round bar is designed to resist different forms of corrosion such as pitting, crevices and chloride stress corrosion cracking.
The material has higher tensile strength and yield strength compared to other alloys. Therefore, it is ideal for structural and load-bearing applications. The material also exhibits excellent fatigue resistance and can be used in cyclic loading applications.
2205 Duplex Round Bar has high toughness even at low temperatures, making it the first choice for cryogenic applications. The material is versatile and is used in pulp and paper, oil and gas, chemical processing and other industries. Regent Steel & Engineering Co. is one of the top suppliers of round steel. They offer precise dimensions, custom surface finishes and competitive pricing for high quality round shapes.
We can produce Duplex 2205 round bar in following forms & shapes:
|
Rod Flat Bars Round Square Channel Bars T-Bars Blocks Precision Ground Bars Rings Hollow Round Rod |
Rectangular Bar Triangle Hex (A/F) Rectangle Half Round Bars Threaded Billet Profiles I/H Bars Forging Ingot |
Duplex 1.4462 round bar Chemical Composition
2205 Duplex Stainless Steel Round Bar Chemical Composition
|
|
Max % |
||||||||||
| Carbon |
0 |
0.03 |
|||||||||
| Silicon |
0 |
1.00 |
|||||||||
| Manganese |
0 |
2.00 |
|||||||||
| Nickel |
4.50 |
6.50 |
|||||||||
| Chromium |
21.00 |
23.00 |
|||||||||
| Molybdenum |
2.50 |
3.50 |
|||||||||
| Nitrogen |
0.08 |
0.20 |
|||||||||
| Phosphorous |
0 |
0.03 |
|||||||||
| Sulphur |
0 |
0.02 |
|||||||||
Duplex 1.4462 round bar Mechanical Properties
| 0.2% Proof Stress | 450 N/mm2 | 65.0ksi |
| Tensile Strength | 680 N/mm2 | 99.0ksi |
| Elongation, 5.65√S0 | 25% | |
| Reduction of area | ||
| Hardness (Rockwell C) | 28 (max) | |
| Impact Strength (Room Temp) | 80J (av) | |
| Impact Strength (-46oC) | 45J (av) | |
| 35J min | ||
Duplex 1.4462 round bar Application
» 2205 Duplex Stainless Steel Round Bar uses in Oil and Gas Pipeline
»2205 Duplex Stainless Steel Round Bar uses in Chemical Industry
» 2205 Duplex Stainless Steel Round Bar uses in Plumbing
» 2205 Duplex Stainless Steel Round Bar uses in Heating
» 2205 Duplex Stainless Steel Round Bar uses in Oil & Gas Industry
» 2205 Duplex Stainless Steel Round Bar uses in Water Supply Systems
» 2205 Duplex Stainless Steel Round Bar uses in Paper & Pulp Industry
» 2205 Duplex Stainless Steel Round Bar uses in Power Plant
» 2205 Duplex Stainless Steel Round Bar uses in Fabrication Industry
» 2205 Duplex Stainless Steel Round Bar uses in General purpose applications
» 2205 Duplex Stainless Steel Round Bar uses in Food Processing Industry
» 2205 Duplex Stainless Steel Round Bar uses in Structural Pipe
» 2205 Duplex Stainless Steel Round Bar uses in Heat Exchangers
» 2205 Duplex Stainless Steel Round Bar uses in also used for other industrial purpose etc.
Duplex 1.4462 round bar Feature
Good general corrosion resistance
High resistance to chloride stress corrosion cracking
high strength
Very good weldability and processability
Good resistance to sulfide stress corrosion
Resistant to chloride pitting and crevice corrosion
Duplex 1.4462 round bar Surface Finish
Duplex 1.4462 round bar Surface Finish

|
CD |
Cold drawn |
P |
Polished |
|
BD |
Bright drawn |
SRE |
Slit rolled edge |
|
CG |
Centreless ground |
HF |
Hot finished |
|
CF |
Cold finished |
HRAP |
Hot rolled annealed and pickled |
|
P&T |
Peeled and turned |
RT |
Rough turned/peeled |
|
ST |
Smooth turned |
PR |
Peeled and reeled |
Duplex 1.4462 round bar Size
OD = outside diameter, ID = inside diameter
|
Size |
Chucked true to OD |
Chucked true to ID |
|||||||
|---|---|---|---|---|---|---|---|---|---|
|
OD, |
ID, |
Max. OD, |
Min. ID, |
Max. OD, |
Min. ID, |
Max. OD, |
Min. ID, |
Max. OD, |
Min. ID, |
|
32 |
20 |
31 |
21.9 |
1.220 |
0.862 |
30 |
21 |
1.185 |
0.827 |
|
32 |
16 |
31 |
18 |
1.220 |
0.709 |
30 |
17 |
1.181 |
0.669 |
|
36 |
25 |
35 |
26.9 |
1.378 |
1.059 |
34.1 |
26 |
1.343 |
1.024 |
|
36 |
20 |
35 |
22 |
1.378 |
0.866 |
34 |
21 |
1.339 |
0.827 |
|
36 |
16 |
35 |
18.1 |
1.378 |
0.713 |
33.9 |
17 |
1.335 |
0.669 |
|
40 |
28 |
39 |
29.9 |
1.535 |
1.177 |
38.1 |
29 |
1.500 |
1.142 |
|
40 |
25 |
39 |
27 |
1.535 |
1.063 |
38 |
26 |
1.496 |
1.024 |
|
40 |
20 |
39 |
22.1 |
1.535 |
0.870 |
37.9 |
21 |
1.492 |
0.827 |
|
45 |
32 |
44 |
33.9 |
1.732 |
1.335 |
43.1 |
33 |
1.697 |
1.299 |
|
45 |
28 |
44 |
30 |
1.732 |
1.181 |
43 |
29 |
1.693 |
1.142 |
|
45 |
20 |
44 |
22.2 |
1.732 |
0.874 |
42.8 |
21 |
1.685 |
0.827 |
|
50 |
36 |
49 |
38 |
1.929 |
1.496 |
48 |
37 |
1.890 |
1.457 |
|
50 |
32 |
49 |
34.1 |
1.929 |
1.343 |
47.9 |
33 |
1.886 |
1.299 |
|
50 |
25 |
49 |
27.2 |
1.929 |
1.071 |
47.8 |
26 |
1.882 |
1.024 |
|
56 |
40 |
55 |
42 |
2.165 |
1.654 |
54 |
41 |
2.126 |
1.614 |
|
56 |
36 |
55 |
38.1 |
2.165 |
1.500 |
53.9 |
37 |
2.122 |
1.457 |
|
56 |
28 |
55 |
30.3 |
2.165 |
1.193 |
53.7 |
29 |
2.114 |
1.142 |
|
63 |
50 |
62 |
51.9 |
2.441 |
2.043 |
61.1 |
51 |
2.406 |
2.008 |
|
63 |
45 |
62 |
47 |
2.441 |
1.850 |
61 |
46 |
2.402 |
1.811 |
|
63 |
40 |
62 |
42.2 |
2.441 |
1.661 |
60.8 |
41 |
2.394 |
1.614 |
|
63 |
36 |
62 |
38.3 |
2.441 |
1.508 |
60.7 |
37 |
2.390 |
1.457 |
|
63 |
32 |
62 |
34.4 |
2.441 |
1.354 |
60.6 |
33 |
2.386 |
1.299 |
|
71 |
56 |
69.9 |
58 |
2.752 |
2.283 |
68.9 |
57 |
2.713 |
2.244 |
|
71 |
45 |
69.9 |
47.3 |
2.752 |
1.862 |
68.6 |
46 |
2.701 |
1.811 |
|
71 |
40 |
69.9 |
42.4 |
2.752 |
1.669 |
68.5 |
41 |
2.697 |
1.614 |
|
71 |
36 |
69.9 |
38.5 |
2.752 |
1.516 |
68.4 |
37 |
2.693 |
1.457 |
|
75 |
60 |
73.8 |
62 |
2.906 |
2.441 |
72.8 |
61 |
2.866 |
2.402 |
|
75 |
50 |
73.8 |
52.2 |
2.906 |
2.055 |
72.6 |
51 |
2.858 |
2.008 |
|
75 |
40 |
73.8 |
42.5 |
2.906 |
1.673 |
72.3 |
41 |
2.846 |
1.614 |
|
80 |
63 |
78.8 |
65 |
3.102 |
2.559 |
77.8 |
64 |
3.063 |
2.520 |
|
80 |
50 |
78.8 |
52.4 |
3.102 |
2.053 |
77.4 |
51 |
3.047 |
2.008 |
|
80 |
45 |
78.8 |
47.5 |
3.102 |
1.870 |
77.3 |
46 |
3.043 |
1.811 |
|
80 |
40 |
78.8 |
42.6 |
3.102 |
1.677 |
77.2 |
41 |
3.039 |
1.614 |
|
85 |
67 |
83.7 |
69.1 |
3.295 |
2.720 |
82.6 |
68 |
3.252 |
2.677 |
|
85 |
55 |
83.7 |
57.4 |
3.295 |
2.260 |
82.3 |
56.0 |
3.240 |
2.205 |
|
85 |
45 |
83.7 |
47.6 |
3.295 |
1.874 |
82.1 |
46.0 |
3.232 |
1.811 |
|
90 |
71 |
88.6 |
73.1 |
3.488 |
2.878 |
87.6 |
72.1 |
3.449 |
2.839 |
|
90 |
63 |
88.6 |
65.3 |
3.488 |
2.571 |
87.3 |
64.0 |
3.437 |
2.520 |
|
90 |
56 |
88.6 |
58.5 |
3.488 |
2.303 |
87.1 |
57.0 |
3.429 |
2.244 |
|
90 |
50 |
88.6 |
52.6 |
3.488 |
2.071 |
87.0 |
51.0 |
3.425 |
2.008 |
|
95 |
75 |
93.5 |
77.3 |
3.681 |
3.041 |
92.4 |
76.2 |
3.641 |
2.997 |
|
95 |
67 |
93.5 |
69.3 |
3.681 |
2.728 |
92.2 |
68.0 |
3.630 |
2.677 |
|
95 |
50 |
93.5 |
52.7 |
3.681 |
2.075 |
91.8 |
51.0 |
3.614 |
2.008 |
|
100 |
80 |
98.5 |
82.3 |
3.878 |
3.240 |
97.4 |
81.2 |
3.835 |
3.197 |
|
100 |
71 |
98.5 |
73.4 |
3.878 |
2.890 |
97.2 |
72.1 |
3.827 |
2.839 |
|
100 |
63 |
98.5 |
65.5 |
3.878 |
2.579 |
97.0 |
64.0 |
3.819 |
2.520 |
|
100 |
56 |
98.5 |
58.7 |
3.878 |
2.311 |
96.8 |
57.0 |
3.811 |
2.244 |
|
106 |
80 |
104.4 |
82.5 |
4.110 |
3.248 |
103.1 |
81.2 |
4.059 |
3.197 |
|
106 |
71 |
104.4 |
73.5 |
4.110 |
2.894 |
103.0 |
72.1 |
4.055 |
2.839 |
|
106 |
63 |
104.4 |
65.7 |
4.110 |
2.587 |
102.7 |
64.0 |
4.043 |
2.520 |
|
106 |
56 |
104.4 |
58.9 |
4.110 |
2.319 |
102.5 |
57.0 |
4.035 |
2.244 |
|
112 |
90 |
110.3 |
92.5 |
4.343 |
3.642 |
109.2 |
91.4 |
4.299 |
3.598 |
|
112 |
80 |
110.3 |
82.6 |
4.343 |
3.252 |
108.9 |
81.2 |
4.287 |
3.197 |
|
112 |
71 |
110.3 |
73.7 |
4.343 |
2.902 |
108.7 |
72.1 |
4.280 |
2.839 |
|
112 |
63 |
110.3 |
65.8 |
4.343 |
2.591 |
108.5 |
64.0 |
4.272 |
2.520 |
|
118 |
90 |
116.2 |
92.7 |
4.575 |
3.650 |
114.9 |
91.4 |
4.524 |
3.598 |
|
118 |
80 |
116.2 |
82.8 |
4.575 |
3.260 |
114.6 |
81.2 |
4.512 |
3.197 |
|
118 |
71 |
116.2 |
73.8 |
4.575 |
2.906 |
114.5 |
72.1 |
4.508 |
2.839 |
|
118 |
63 |
116.2 |
66.0 |
4.575 |
2.598 |
114.2 |
64.0 |
4.496 |
2.520 |
|
125 |
100 |
123.1 |
102.7 |
4.846 |
4.043 |
121.9 |
101.5 |
4.799 |
3.996 |
|
125 |
90 |
123.1 |
92.8 |
4.846 |
3.654 |
121.7 |
91.4 |
4.791 |
3.598 |
|
125 |
80 |
123.1 |
82.9 |
4.846 |
3.264 |
121.4 |
81.2 |
4.780 |
3.197 |
|
125 |
71 |
123.1 |
74.0 |
4.846 |
2.913 |
121.3 |
72.1 |
4.772 |
2.839 |
|
132 |
106 |
130.0 |
108.8 |
5.118 |
4.283 |
128.8 |
107.6 |
5.071 |
4.236 |
|
132 |
90 |
130.0 |
93.0 |
5.118 |
3.661 |
128.4 |
91.4 |
5.055 |
3.598 |
|
132 |
80 |
130.0 |
83.1 |
5.118 |
3.272 |
128.1 |
81.2 |
5.043 |
3.197 |
|
132 |
71 |
130.0 |
74.2 |
5.118 |
2.921 |
121.2 |
72.1 |
5.035 |
2.839 |
|
140 |
112 |
137.9 |
115 |
5.429 |
4.528 |
136.6 |
113.7 |
5.378 |
4.476 |
|
140 |
100 |
137.9 |
103.1 |
5.429 |
4.059 |
136.3 |
101.5 |
5.366 |
3.996 |
|
140 |
90 |
137.9 |
93.2 |
5.429 |
3.669 |
136.1 |
91.4 |
5.358 |
3.598 |
|
140 |
80 |
137.9 |
83.3 |
5.429 |
3.280 |
135.8 |
81.2 |
5.346 |
3.197 |
|
150 |
125 |
147.7 |
128.1 |
5.815 |
5.043 |
146.5 |
126.9 |
5.768 |
4.996 |
|
150 |
106 |
147.7 |
109.3 |
5.815 |
4.303 |
146 |
107.6 |
5.748 |
4.236 |
|
150 |
95 |
147.7 |
98.4 |
5.815 |
3.874 |
145.7 |
96.4 |
5.736 |
3.795 |
|
150 |
80 |
147.7 |
83.6 |
5.815 |
3.291 |
145.3 |
81.2 |
5.720 |
3.197 |
|
160 |
132 |
157.6 |
135.3 |
6.205 |
5.327 |
156.3 |
134 |
6.154 |
5.276 |
|
160 |
122 |
157.6 |
125.4 |
6.205 |
4.937 |
156 |
123.8 |
6.142 |
4.874 |
|
160 |
112 |
157.6 |
115.5 |
6.205 |
4.547 |
155.8 |
113.7 |
6.134 |
4.476 |
|
160 |
90 |
157.6 |
94.0 |
6.205 |
3.701 |
155.2 |
91.4 |
6.110 |
3.598 |
|
170 |
140 |
167.4 |
143.5 |
6.591 |
5.650 |
166 |
142.1 |
6.535 |
5.594 |
|
170 |
130 |
167.4 |
133.6 |
6.591 |
5.260 |
165.8 |
132 |
6.528 |
5.197 |
|
170 |
128 |
167.4 |
131.6 |
6.591 |
5.181 |
165.7 |
130 |
6.524 |
5.118 |
|
170 |
118 |
167.4 |
121.7 |
6.591 |
4.791 |
165.5 |
119.8 |
6.516 |
4.717 |
|
170 |
106 |
167.4 |
109.8 |
6.591 |
4.323 |
165.2 |
107.6 |
6.504 |
4.236 |
|
170 |
100 |
167.4 |
103.9 |
6.591 |
4.091 |
165 |
101.5 |
6.496 |
3.996 |
|
180 |
150 |
177.3 |
153.6 |
6.980 |
6.047 |
176 |
152.3 |
6.929 |
5.996 |
|
180 |
140 |
177.3 |
143.7 |
6.980 |
5.657 |
175.7 |
142.1 |
6.917 |
5.594 |
|
180 |
125 |
177.3 |
128.9 |
6.980 |
5.075 |
175.3 |
126.9 |
6.902 |
4.996 |
|
180 |
100 |
177.3 |
104.1 |
6.980 |
4.098 |
174.7 |
101.5 |
6.878 |
3.996 |
|
190 |
160 |
187.1 |
163.8 |
7.366 |
6.449 |
185.7 |
162.4 |
7.311 |
6.394 |
|
190 |
150 |
187.1 |
153.9 |
7.366 |
6.059 |
185.5 |
152.3 |
7.303 |
5.996 |
|
190 |
132 |
187.1 |
136 |
7.366 |
5.354 |
185.1 |
134 |
7.287 |
5.276 |
|
200 |
170 |
197.0 |
173.9 |
7.756 |
6.846 |
195.6 |
172.6 |
7.701 |
6.795 |
|
200 |
160 |
197.0 |
164 |
7.756 |
6.457 |
195.4 |
162.4 |
7.693 |
6.394 |
|
200 |
150 |
197.0 |
154.1 |
7.756 |
6.067 |
195.2 |
152.3 |
7.685 |
5.996 |
|
200 |
140 |
197.0 |
144.2 |
7.756 |
5.677 |
194.9 |
142.1 |
7.673 |
5.594 |
|
212 |
170 |
208.8 |
174.2 |
8.220 |
6.858 |
207.2 |
172.6 |
8.157 |
6.795 |
|
212 |
150 |
208.8 |
154.4 |
8.220 |
6.079 |
206.6 |
152.3 |
8.133 |
5.997 |
|
212 |
130 |
208.8 |
134.6 |
8.220 |
5.299 |
206.2 |
132 |
8.118 |
5.197 |
|
224 |
180 |
220.6 |
184.4 |
8.685 |
7.260 |
218.9 |
182.7 |
8.618 |
7.193 |
|
224 |
140 |
220.6 |
144.8 |
8.685 |
5.701 |
217.9 |
142.1 |
8.579 |
5.594 |
|
236 |
190 |
232.4 |
194.6 |
9.150 |
7.661 |
230.7 |
192.9 |
9.083 |
7.594 |
|
236 |
150 |
232.4 |
155.0 |
9.150 |
6.102 |
229.7 |
152.3 |
9.043 |
5.996 |
|
250 |
200 |
246.2 |
204.9 |
9.693 |
8.067 |
244.3 |
203.0 |
9.618 |
7.992 |
|
275 |
200 |
268.9 |
205.4 |
10.587 |
8.087 |
266.5 |
203.0 |
10.492 |
7.992 |
Duplex 1.4462 round bar Packing & Delivery
Duplex 1.4462 round bar Packing & Delivery

Customer Visit

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide
FAQ
Q:What is your delivery time ?
A: Our delivery time is about one week, timing according to the number of customers.
Q: Can I get your best price?
A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.
Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.
Q: About the product price of UNS S30100 stainless steel?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
contact us
contact us
Hot Tags: Duplex 1.4462 round bar, China Duplex 1.4462 round bar suppliers, duplex stainless steel user, Duplex 2003 Stainless Steel Plate, duplex stainless steel exchange, duplex stainless steel fabrication, duplex stainless steel availability, duplex stainless steel reducer