UNS N07750 Pipe
video

UNS N07750 Pipe

UNS N07750 is a precipitation-hardenable nickel-chromium alloy that offers excellent corrosion and oxidation resistance along with high strength at elevated temperatures. UNS N07750 pipes are used in various high-temperature applications where these properties are required.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n07750 pipe in China. If you're going to wholesale high quality uns n07750 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

UNS N07750 Pipe

 

Inconel UNS N07750 Pipe Features

UNS N07750 alloy pipe is mainly a nickel-based superalloy which is age-strengthened with γ[Ni3(Al, Ti, Nb)] phase. It has good corrosion resistance and oxidation resistance below 980℃, and below 800℃ It has high corrosion resistance. It has good relaxation resistance below 540°C, as well as good formability and weldability. This alloy is mainly used for the manufacture of aircraft engines that work below 800°C and require high strength. . Springs can also be used to manufacture steam turbine turbine blades and other parts, such as plates, strips, bars, forgings, rings, wires, pipes, etc.

UNS N07750 Pipe Heat Treatment Process

The solution heat treatment system for plates, strips and pipes in the supply state is 980℃±15℃, air cooling. For the intermediate heat treatment system of materials and parts, the following processes can be selected for heat treatment.
Annealing: 955~1010℃, water cooling.
Annealing of welded parts before welding: 980℃, 1h.
Stress relief annealing of welded parts: 900℃, moisturizing for 2h.
Stress relief annealing: 885℃±15℃, 24h, air cooling.

Packing&Delivery

 

 

 

 

UNS N07750 Steel Bar

Hot Tags: uns n07750 pipe, China uns n07750 pipe suppliers, aerospace alloy, durable alloy, reliable alloy, strong alloy, wear resistant alloy, oxidation resistant alloy