Seamless Welded 400 401 Monel Pipes
Sizes: 1/2" - 12" OD, Gauges: 25 SWG - 10 SWG
OD: 6.35 to 114.3 mm O.D
Thickness: 0.8 - 12.7 mm
Length: Up to 26 meters
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of seamless welded 400 401 monel pipes in China. If you're going to wholesale high quality seamless welded 400 401 monel pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Welded 400 401 Monel Pipes introduce
Seamless 400 401 Monel Pipes


Monel 400 (UNS N04400/W.Nr. 2.4360) is a nickel-copper alloy (approximately 67% nickel - 23% copper) that is resistant to high-temperature seawater and steam, as well as salt and alkaline solutions. Alloy 400 is a solid solution alloy that can only be hardened by cold working. This nickel alloy has properties such as good corrosion resistance, good weldability, and high strength. Low corrosion rates in fast-moving saltwater or seawater, excellent resistance to stress corrosion cracking in most freshwaters, and resistance to a wide range of corrosive conditions make it widely used in marine applications and other non-oxidizing chloride solutions.
UNS N04401 Monel 401 is a high-performance alloy composed primarily of nickel and copper. It is designed to combine the superior strength of nickel with the corrosion resistance of copper, making it a durable and versatile choice for industries operating in demanding environments. Monel 401 alloy is known for its electrical and thermal conductivity, which makes it suitable for specialty applications such as thermocouples and electrical connectors.
Due to its unique composition and strong physical properties, Monel 401 alloy is a reliable material for a variety of industrial applications.
Seamless Welded 400 Monel Pipes



monel 400 Welded Pipes Chemical Composition
The chemical composition of Monel 400 Alloy is given in the following table.
| Element | Content (%) |
|---|---|
| Nickel, Ni | Remainder |
| Copper, Cu | 28-34 |
| Iron, Fe | 2.5 max |
| Manganese, Mn | 2 max |
| Silicon, Si | 0.5 max |
| Carbon, C | 0.3 max |
| Sulphur, S | 0.024 |
Super Alloys Monel 401 Chemical
| Aluminum | 0.2 - 0.8 |
|---|---|
| Boron | 0.006 max |
| Carbon | 0.08 max |
| Chromium | 17 - 21 |
| Cobalt | 1 max |
| Copper | 0.3 max |
| Iron | Balance |
| Manganese | 0.35 max |
| Molybdenum | 2.8 - 3.3 |
| Nickel | 50 - 55 |
| Niobium | 4.75 - 5.5 |
| Phosphorus | 0.015 max |
| Silicon | 0.35 max |
| Sulphur | 0.015 max |
| Titanium | 0.65 - 1.15 |
GNEE Group Factory Environment
Seamless 400 alloy Pipes

GNEE Group Product Packaging
Seamless Welded 401 Pipes

FAQ
Q: Can I get samples before order ?
A: Yes, of course.We can produce by your samples or technical drawings ;
Q: Can I go to your factory to visit?
A: Of course, we welcome customers from all over the world to visit our factory ;
Q: What kind of work does your company do?
A: Our company is a professional manufacturer.We mainly produces stainless steel sheet, stainless steel coil, stainless steel pipe, stainless steel bars and so on.
Q: How can you assure your quality?
1.We can provide you certificate of quality accordingly.
2.We are willing to accept the third party inspection, such as SGS,BV,CE and so on.
Hot Tags: Seamless Welded 400 401 Monel Pipes, China Seamless Welded 400 401 Monel Pipes suppliers, Cold Rolled Inconel 625 Alloy Seamless Pipe, Nickel Alloy Coil B2, Alloy Steel 600 plate, Ni36CrTiAl Plate, Hastelloy C 22 Alloy Steel Flange, Uns N06600 Alloy tubing
You Might Also Like
Send Inquiry