Hastelloy Metal C22 Mirror Alloy Coil
video

Hastelloy Metal C22 Mirror Alloy Coil

Hastelloy C-22 Coil

Thickness
2.5 mm - 10.0 mm

Length
2000 mm, 2440 mm, 3000 mm, 5800 mm, 6000 mm, etc.

Width
610 mm - 2000 mm
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy metal c22 mirror alloy coil in China. If you're going to wholesale high quality hastelloy metal c22 mirror alloy coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

 

Hastelloy Metal C22 Mirror Alloy Coil Description

Chemical composition of MonelR405 nickel-copper alloy strip

 

Gnee Steel Hastelloy C22 Mirror Alloy Coil

Hastelloy C22 Coil, the Ultimate Choice for Corrosion-Resistant Applications. Our Hastelloy C22 Coil is designed to withstand the most challenging environments, ensuring superior durability and reliability in a wide range of industrial sectors.
Hastelloy C22 Coil is made from a low-carbon nickel-based alloy containing key elements such as nickel, chromium and molybdenum. This unique composition gives it excellent resistance to a wide range of corrosive substances, making it an ideal choice for critical applications where corrosion is a concern.
Our Hastelloy C22 Coil is widely used in industries such as chemical, petrochemical, and pharmaceutical. Its superior corrosion resistance makes it the first choice for handling corrosive media and harsh conditions.

Hastelloy C-22 Coil Features

Hastelloy C-22 coils offer several key features that make them highly suitable for a wide range of industrial applications.
Corrosion resistance: Hastelloy C-22 coils exhibit excellent corrosion resistance to all corrosive, oxidizing and deoxidizing environments.
High performance: These coils have standardized mechanical properties that allow them to be used in both high and low temperature environments.
Versatility: Hastelloy C-22 coils are easy to fabricate and install as they can be bent, welded and machined, whereas stainless steel cannot bend easily.
Durability: They offer excellent resistance to pitting, crevice corrosion and stress corrosion cracking, allowing them to be used for long periods in harsh environments.
Hastelloy C-22 coils offer excellent resistance to oxidation and corrosion, making them ideal for extreme environments.

Hastelloy C22 Coils specifications

Hastelloy C22 Coils Specifications
Specifications ASTM / ASME SB575
Size 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Thickness 0.1mm to 12 mm Thk
Form Coils, Foils, Rolls, Plain Coils, Shim Coils, Strip, Flats, Blank (Circle), Ring (Flange)
Finish Hot rolled Coils (HR), Cold rolled Coils (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Hastelloy C22 Coils Chemical Composition

Grade C Mn Si S Co Ni Cr Fe Mo P
Hastelloy C22 0.010 max 0.50 max 0.08 max 0.02 max 2.50 max 50.015 min 20.00 – 22.50 2.00 – 6.00 12.50 – 14.50 0.02 max

Hastelloy C22 Coils Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy C22 8.69 g/cm3 1399 °C (2550 °F) Psi – 1,00,000 , MPa – 690 Psi – 45000 , MPa – 310 45 %

Hastelloy C22 Mirror Coil Packaging

Hastelloy C22 Mirror Coil

Hastelloy Metal C22 Mirror Alloy Coil

Metal C22 Mirror Alloy Coil Factory Environment

Metal C22 Mirror Alloy Coil

Hastelloy Metal C22 Mirror Alloy Coil

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel is a supplier of Hastelloy Metal C22 Mirror Alloy Coil, with products covering tubes: Seamless tubes: Size: 4 - 219 mm; Thickness: 0.5 - 20 mm; Welded tubes: Size: 5.0 - 1219.2 mm; Thickness: 0.5 - 20 mm, Plates: Plate thickness 0.1 to 100 mm; Plate width 10-2500 mm, Strips, Alloy round bar sizes: diameter 3-800 mm;, Flat bar sizes: thickness 2-100 mm; Width: 10-500 mm, Hexagonal bar sizes: 2-100 mm;, Wire and extruded profiles. We work with steel mills to provide customers with 625 alloy, and its products meet or exceed many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Hastelloy Metal C22 Mirror Alloy Coil, Tubes, Pipes, Sheets, Strips, Plates, Round Bars, Flat Bars, Forged Billets, Hexagons, Wires and Extruded Profiles. Feel free to contact us for a quote at ss@gneesteel.com