Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel based alloy 201 steel sheet in China. If you're going to wholesale high quality nickel based alloy 201 steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Nickel 201 is a commercially pure nickel alloy similar to Nickel 200 but with a lower carbon content (0.02% max), making it especially suitable for applications requiring excellent corrosion resistance in high-temperature, reducing, and neutral environments. Its low carbon content reduces the risk of graphite precipitation, which can occur in higher carbon content alloys, making Nickel 201 more resistant to embrittlement at high temperatures.
Key Features of Nickel 201
Outstanding Corrosion Resistance: Performs well in reducing and neutral environments, particularly in handling alkalis and acids.
High Temperature Stability: Suitable for applications up to approximately 600°C (1112°F) without becoming brittle.
Good Mechanical Properties: Offers excellent ductility, making it easy to form, weld, and machine.
Low Carbon Content: Designed to prevent embrittlement and withstand high-temperature exposure without losing mechanical integrity.

Specifications
| Specification | Details |
|---|---|
| Chemical Composition | |
| Nickel (Ni) | ≥99.0% |
| Carbon (C) | ≤0.02% |
| Silicon (Si) | ≤0.35% |
| Copper (Cu) | ≤0.25% |
| Iron (Fe) | ≤0.40% |
| Mechanical Properties | |
| Tensile Strength | ≥345 MPa |
| Yield Strength | ≥103 MPa |
| Elongation | ≥40% |
| Dimensions | |
| Thickness | 0.5mm - 80mm (plate); 1mm - 60mm (rod) |
| Width | 1000mm - 2000mm (plate) |
| Length | 2000mm - 6000mm (plate, customizable) |
| Form | Plate, rod, tube, strip, wire |

Applications
Chemical Processing: Ideal for handling caustic soda, acid solutions, and for equipment operating in high temperatures.
Electronics Industry: Used for electronic and electrical parts, such as battery connectors and anodes, where high conductivity is required.
Heat Exchangers: Suitable for high-temperature components in furnaces, heat exchangers, and gas turbines.
Food and Pharmaceutical: Used for processing and storage equipment due to its corrosion resistance and purity.
Aerospace: Components requiring a stable material under heat and chemical exposure.
Nickel 201's low carbon composition and excellent corrosion resistance make it ideal for high-temperature environments and critical applications in industries that require materials with high integrity and resistance to embrittlement.