Mn13 Nm500 Ar500 Alloy Steel Plate Wear Resistant Steel Plate
video

Mn13 Nm500 Ar500 Alloy Steel Plate Wear Resistant Steel Plate

Model NO. steel Plate Type Wear Resistant Plate Technology Hot Rolling Lenght Custmization Hardness Range 360hb-600hb Main Hardness 400hb 450hb 500hb Cutting and Bending Service Yes Ready Stock Yes Transport Package Seaworthy Packaging Specification thickness: 3mm-80mm
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of mn13 nm500 ar500 alloy steel plate wear resistant steel plate in China. If you're going to wholesale high quality mn13 nm500 ar500 alloy steel plate wear resistant steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Mn13 Nm500 Ar500 Alloy Steel Plate Wear Resistant Steel Plate

Product Description

NM400 NM500 wear resistant steel plate wear plates
Abrasion Resisant Plate AR400 AR500
Abrasive resistant steel
Hard steel plate
hard 500 hard 400
steel plate cutting and bending

Product Descrition
1.Production Process
1)Steelmaking process Flow Chart
Blast Furance+Hot Metal Ladle Truck+KR Hot Metal Treatment+Converter+LF Refining Furnace+RH Vacuum Degassing Furance+Con-cast

2.Rolling Process Flow Chart
Reheating Furance+High-pressure Water Descaling+Edger Mill+Roughing Mill+Finishing Mill+Accelerated cooling+Hot Leveler+Marking and Spray Printing+Cooling Bed+On-line UT+Crop Shear+Double-side Trimming Shear+Cut-to-length Shear+Measurement+Marking and Spray Printing+Cold Leveler/Heat treatment

3.Heat-Treatment Flow Chart
Plate+Shot Blasting+Quenching Furance+Quenching Machine+Tempering Furance+Warm Leveler+Cooling Bed+Cutting+Cold Leveler+Finishing&Packaging

4.Thickness and Width
Thickness:4.5mm-150mm
Width:1600mm-4100mm

5.Main Grade
Germany:XAR400,XAR450,XAR500,XAR600,Dillidur400,Dillidur500
Belgium:QUARD400,QUARD450,QUARD500
France:FORA400,FORA500,Creusabro4800,Creusabro8000
Baosteel:B-HARD360,B-HARD400,B-HARD450,B-HARD500
HBIS:NM360,NM400,NM450,NM500
Finland:RAEX400,RAEX450,RAEX500
Japan:JFE-EH360,JFE-EH400,JFE-EH500,WEL-HARD400,WEL-HARD500

6.Chemical Composition&Property

Grade c Si Mn P S Al Cr+Ni+Mo Nb+V+Ti
NM400 0.10-0.40 0.20-0.40 1.00-2.00 Max 0.015 Max 0.003 Min 0.020 Max 0.9 Trace Amount
NM450 0.10-0.40 0.20-0.40 1.00-2.00 Max 0.015 Max 0.003 Min 0.020 Max 1.2
NM500 0.10-0.40 0.20-0.45 1.00-2.00 Max 0.015 Max 0.003 Min 0.020 Max 1.5
NM550 0.10-0.50 0.20-0.45 1.00-1.50 Max 0.015 Max 0.003 Min 0.020 Max 2.0
NM600 0.10-0.50 0.20-0.45 1.00-1.50 Max 0.015 Max 0.003 Min 0.020 Max 2.5
XCHD400 0.10-0.30 0.20-0.40 1.00-2.00 Max 0.015 Max 0.003 Min 0.020 Max 0.1
XCHD450 0.10-0.40 0.20-0.40 1.00-2.00 Max 0.015 Max 0.003 Min 0.020 Max 0.9
XCHD500 0.10-0.40 0.20-0.45 1.00-2.00 Max 0.015 Max 0.003 Min 0.020 Max 1.5


7.

Grade Size(mm) RP0.2(Mpa) Rm(Mpa) A50(%) AKV,(ºC) KV2(J) HBW
NM400 100 1233 1337 15 -20 35 37 42 415
NM450 60 1345 1434 9.5 -20 72 59 58 455
NM500 50 1608 1706 10.5 -20 43 50 45 495
XCHD400 35 1025 1161 17.5 -40 52 45 40 413
XCHD450 30 1281 1400 10.5 -40 45 48 52 453
XCH500 6 1465 1529 13.5 -40 24 24 22 515


8.Cerifications
9 Classification Society
ISO 9001 Certified

9.Packaging&Shipping
Seaworthy packaging by container or bulk cargo vessel
Delievery time:stock size within 7days;new material within 40days
10.Our services
We can cut and bend steel plate according to customer's requriement or drawing,packaging according to customers' request
11.Application
By adopting the combined chemical composition design of low carbon,low sulfur,low phosphorous and micro-alloy,by applying the offline quenching and other advanced automation technologies,our wear resistant(Abrasion Resisant) plate are popular at home and abroad. Mainly used for thermal Power plant,Coal Mines ,Cement Mills,Loading Machinery,Mining Machinery,Project Machinery.Metallurgical Machinery,Wear resistant plate also can be applied in Sand Mill Cylindrical Shell, Vane, Mechanical Parts used in yard and port, Bearing Structure Parts etc.

Hot Tags: mn13 nm500 ar500 alloy steel plate wear resistant steel plate, China mn13 nm500 ar500 alloy steel plate wear resistant steel plate suppliers, product alloy, corrosion resistant alloy, construction alloy, special alloy, industrial alloy, advanced alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry