INCONEL nickel-iron-chromium alloy 706 (UNS N09706) is a precipitation-hardenable alloy that provides high mechanical strength in combination with good fabricability. The characteristics of the alloy are similar to those of INCONEL alloy 718 except that alloy 706 is more readily fabricated, particularly by machining.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel uns n09706 alloy bar in China. If you're going to wholesale high quality inconel uns n09706 alloy bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel UNS N09706 Alloy Bar

Product Introduction

INCONEL nickel-iron-chromium alloy 706 (UNS N09706) is a precipitation-hardenable alloy that provides high mechanical strength in combination with good fabricability. The characteristics of the alloy are similar to those of INCONEL alloy 718 except that alloy 706 is more readily fabricated, particularly by machining.

The substantial nickel and chromium contents provide good resistance to oxidation and corrosion. The primary precipitation-hardening constituents of the alloy are niobium and titanium. The aluminum content also contributes to the hardening response.

The precipitation-hardening system in INCONEL alloy 706 provides the desirable characteristic of delayed hardening response during exposure to precipitation temperatures. That characteristic gives the alloy excellent resistance to postweld strain-age cracking.