GH3039 3044 High Heat Stainless Steel Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh3039 3044 high heat stainless steel pipe in China. If you're going to wholesale high quality gh3039 3044 high heat stainless steel pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GH3039 3044 High Heat Stainless Steel Pipe suppliers Description
GH3039 3044 high temperature metal alloys pipe video
GNEE STEEL GROUP supplies GH3039 3044 High Heat Stainless Steel Pipe for you
GH3039 High Heat Stainless Steel Pipe
Same grade: ЭИ602, XH75MБГЮ
Standard: GJB3165-98,GJB1952-94,GJB3318-98,GB/T15062-94
Common supply form: Rod, plate, strip, pipe
| Nickel GH3030 Superalloy Pipe GH3030 High Temperature Alloy Tube | |
| Outside Diameter | 10.3-426mm |
| Wall Thickness | 1.24-40.49mm |
| Length | Up to 25m |
| Standard | ASTM B163, ASTM B167, ASTM B407, ASTM B444, ASTM B622, ASTM B677, ASTM B829,etc. |
Specifications : GB/T 14994
Grade: GH3044
Length : Required Length
Round Bar Diameter : 4.00 mm to 400 mm
Bright Bar : 4mm – 150mm,
Surface Finish : Black, Bright, Polished
Form : Round, Billet, Ingot, Forging Etc.
GH3039 3044 High Heat Stainless Steel Pipe Specification
| GH3039 Thermal Properties | ||||||||||||
| (1),GH3039 Thermal Conductivity : | ||||||||||||
| θ/ºC | 100 | 200 | 300 | 400 | 500 | 600 | 700 | 800 | 900 | |||
| λ/(W/(m · ºC)) | 13.8 | 15.5 | 17.2 | 18.8 | 20.5 | 21.8 | 23.4 | 25.1 | 26.8 | |||
| (2),GH3039 Specific Heat Capacity: | ||||||||||||
| θ/ºC | 150 | 200 | 300 | 400 | 500 | 600 | 700 | 800 | ||||
| c/(J/(kg.K)) | 544 | 574 | 636 | 645 | 762 | 779 | 921 | 1047 | ||||
| (3),GH3039 Coefficient of Linear Thermal Expansion: | ||||||||||||
| θ/ºC | 20-100 | 20-200 | 20-300 | 20-400 | 20-500 | 20-600 | 20-700 | 20-800 | 20-900 | 20-1000 | ||
| a/10-6ºC-1 | 11.5 | 12.4 | 13.2 | 13.5 | 13.8 | 14.3 | 14.9 | 15.3 | 15.8 | 16.4 | ||
| GH3044 Chemical Composition and Mechanical properties: |
| Grade | C | Mn | P | S | Si | Cr | Fe | Al | Mo | Ti | W |
| GH3044 | 0.10 max | 0.50 max | 0.013 max | 0.013 max | 0.80 max | 23.5 – 26.5 | 4.0 max | 0.5 max | 1.5 max | 0.3 – 0.7 | 13.0 – 16.0 |
GH3039 3044 high temperature nickel alloys pipe


GH3039 is an iron-nickel alloy composed of nickel, chromium, molybdenum, iron, cobalt, copper, manganese and silicon. This alloy has excellent mechanical and thermal properties, making it ideal for use in high temperature, pressure and corrosive environments. GH3039 is widely used in aerospace, chemical industry, energy, nuclear industry and other fields.
GH3044 is a Ni-Cr-based solid solution strengthened deformed high-temperature alloy with a service temperature below 900 degrees Celsius. The alloy contains large amounts of tungsten and small amounts of aluminum and titanium. The alloy has high plasticity and moderate thermal strength, and has excellent oxidation resistance and good new functions in stamping and welding processes.
Products technology


Products packing

Customer Case
customer visit

FAQ
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.
Q: About the product price of GH3039 3044 high heat stainless steel pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Contact Us
Address
No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China
Phone
+86-15824687445
ss@gneesteel.com
Skype
mmkelly1314
Whatsapp/Wechat
+86 15824687445
Hot Tags: gh3039 3044 high heat stainless steel pipe, China gh3039 3044 high heat stainless steel pipe suppliers, Casting High Temperature Alloy