ASTM B725 UNS N02200 Welded Nickel Pipe
video

ASTM B725 UNS N02200 Welded Nickel Pipe

Name:ASTM B725 UNS N02200 Welded Nickel Pipe
Approximate grades: NO2200, Nickel200, Ni200, N6
Section Shape:Round
OD:12.7mm--273mm
W.T.:1.24mm--15.09mm
Substrate shape: wire/strip/rod/tube/plate
Implementation standard: GB/T5235
Application areas: industrial field, marine ships
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b725 uns n02200 welded nickel pipe in China. If you're going to wholesale high quality astm b725 uns n02200 welded nickel pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM B725 UNS N02200 Nickel Alloy Welded Pipe is suitable for welded and annealed or welded and stress relieved nickel pipe primarily for general corrosion service and mechanical applications.


UNS N02200 Welded Steel Pipe Processing and Welding Properties
UNS N02200 has good cold and hot working properties and is suitable for various forms of mechanical processing, such as forging, stamping, drawing, bending and spinning. Including gas welding, argon arc welding, laser welding, etc., and the joint performance after welding is good, without obvious brittleness and hot cracking problems.

Nickel 200 Alloy Pipe Specification

ASTM B725 Nickel 200 Welded Pipe Specifications

Specifications ASTM B 725 / 730, ASME SB 725 / 730
Dimensions ASTM, ASME and API
Size 1/8″NB TO 30″NB IN
Specialized in Large Diameter Size
Type ERW / Welded / Fabricated / LSAW Pipes
Form Round, Square, Rectangular, Hydraulic Etc.
Schedule SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Nickel Alloys 200 Products Display

Nickel Alloy 200 ASTM B725 Welded Pipe

Nickel Alloy 200 ASTM B725 Welded Pipe

Why choosing GNEE

GNEE has a domestically advanced large-scale LG320 fully automatic cold rolling mill, which can produce a series of standard terminal products with a diameter of 219mm-0325mm. It has large production capacity, uniform geometric dimensions, no deflection, no defects inside and outside the products, high smoothness, and can meet the requirements of various inspection standards.

please contact us for a quote! ss@gneesteel.com

Nickel Alloy UNS N02200 Pipes PRODUCTS TESTING

Nickel 200 high precision Tube

nickel  200 Alloy Manufacturer

Nickel  200 Alloy Manufacturer

Nickel DIN 2.4066 Pipe Supplier, Stockist

 Superalloys 200 Pipe Supplier, Stockist

FAQ

1.Q.How can I trust you?
A. We think honesty is the core of our company, you can come to know it personally so that you can check our credit.

2. Q: What services do you provide?
A: Customized service for each customer, please feel free to contact us!

3.Q: How do your guarantee the quality?
A: Before mass production, there must be pre-production samples; before shipment, there must be final inspection.

Hot Tags: astm b725 uns n02200 welded nickel pipe, China astm b725 uns n02200 welded nickel pipe suppliers, Ni36CrTiAl Plate, Hastelloy C 22 Alloy Steel Flange, Cold Rolled Inconel 625 Alloy Seamless Pipe, 2 4668 Nickel Alloy Steel Coil, Uns N06600 Alloy tubing, Nickel Alloy Coil B2

Send Inquiry

whatsapp

Phone

E-mail

Inquiry