600 Nickel Iron Alloy Tubing
video

600 Nickel Iron Alloy Tubing

Available Formats
GNEE Group offers Nickel Alloy Inconel 600 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 600 nickel iron alloy tubing in China. If you're going to wholesale high quality 600 nickel iron alloy tubing made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

600 Nickel Iron Alloy Tubing introduce

600 Nickel Iron Alloy Tubing

600 Nickel Iron Alloy Tubing600 Nickel Iron Alloy Tubing

Alloy 600 is a nickel-chromium-iron solid solution strengthened alloy with a nominal chemical composition of 72% nickel, 16% chromium, and 8% iron. It is commonly known by the trade name Inconel 600 and the generic name UNS N06600. Alloy 600 has good corrosion resistance in many media and excellent oxidation resistance at elevated temperatures.

Characteristics

Corrosion graphic

Corrosion Resistance

Alloy 600 has outstanding corrosion resistance imparted by the dual corrosion fighting power of chromium and nickel. Chromium resists corrosion from oxidizing media while nickel defends against attack from many reducing agents. Alloy 600 exhibits good corrosion resistance in reducing acids, mildly oxidizing acids, high purity water, and other media. However, Alloy 600 is not suitable for strong oxidizing acids such as hot nitric acid. It is essentially immune to chloride stress corrosion cracking.

Service Temperature

Elevated Temperature Resistance

Alloy 600 provides excellent oxidation resistance at temperatures up to 2150°F (1177°C). However, it is susceptible to sulfidation attack.

Mechanical Properties

Inconel 600 Mechanical Properties

Alloy 600 can be provided in the lower strength, annealed condition, or strengthened through the pilger process. Alloy 600 maintains excellent toughness even in the higher strength conditions and maintains toughness at cryogenic temperatures.

heat treatment logo

Inconel 600 Heat Treatment

While Alloy 400 cannot be strengthened by heat treating, annealing or stress relieving are commonly used after hot working or cold working operations. Stress-relieving is conducted at 1400°F - 1600°F (760°C - 871°C). Stress-relieving is performed after cold working to reduce residual stress and prevent distortion. Annealing is performed at 1700°F - 1900°F (927°C - 1038°C) to restore full softness.

Workability

Workability

Alloy 600 has good hot and cold workability in the annealed condition. Hot-working should be done above 1600°F (871°C) to ensure adequate ductility, while cold work should be performed below 1200°F (649°C).

Chemical Composition Of Alloy 600 Tube

Grade Mn C S Si Fe Ni Cr Cu
Inconel 600 Pipes minimum – – – – 6.0 72.0 14.0 –
maximum 1.0 0.15 0.015 0.5 10.0 – 17.0 0.5

GNEE Group Product Packaging

600 Nickel Iron Alloy Tubing

600 Nickel Iron Alloy Tubing

GNEE Group Factory Environment

600 Inconel metal polished tube

Inconel 600 alloy seamless tube

 

FAQ

1. how can we guarantee quality?
Always a pre-production sample before mass production;
Always final Inspection before shipment;
2.what can you buy from us?
Seamless pipe,stainless steel,carbon steel,Square tube,Profile
3. why should you buy from us not from other suppliers?
GNEE Steel Co., Ltd. is an enterprise specializing in the production of high-quality steel pipes, mainly producing stainless steel, seamless pipes, carbon steel, galvanized, profiles, etc. it is a professional one-stop steel product supplier.

Hot Tags: 600 Nickel Iron Alloy Tubing, China 600 Nickel Iron Alloy Tubing suppliers, 2 4668 Nickel Alloy Steel Coil, Uns N06600 Alloy tubing, Hastelloy C 22 Alloy Steel Flange, Nickel Alloy Coil B2, Monel 400 Alloy Steel Sheet, Ni36CrTiAl Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry