4140 Hot Forged Rolled Steel Round Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 4140 hot forged rolled steel round bar in China. If you're going to wholesale high quality 4140 hot forged rolled steel round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
4140 Hot Forged Rolled Steel Round Bar
1: 4140 steel introduction
AISI SAE 4140 alloy steel is a chromium molybdenum alloy steel specification widely used in general purpose high tensile steel for components, like axles, shafts, bolts, gears and other applications. Similar to alloy grade AISI 4130 chrome moly alloy steel but with a slightly higher carbon content. The higher carbon content of AISI 4140 steel gives greater strength and heat treatment capabilities in comparison to AISI / ASTM 4130 alloy steels, however it does have inferior weldability characteristics..
2: 4140 Steel equivalent
| Country | Japan | Germany | Britain | USA | China | Australia |
| Standard | JIS G4105 | DIN 17200 | BS970 | ASTM A29 | GB/T 3077 | AS 1444 |
| Grade | SCM440 | 42CrMo4/1.7225 | EN19/709M40 | 4140 | 42CrMo | 4140 |
3: 4140 steel chemical composition
| Grade | C | Si | Mn | P | S | Cr | Mo | Ni |
| 4140 | 0.38-0.43 | 0.15-0.35 | 0.75-1.0 | 0.035 | 0.04 | 0.8-1.1 | 0.15-0.25 | |
| 42CrMo4 | 0.38-0.45 | 0.4 | 0.6-0.9 | 0.035 | 0.035 | 0.9-1.2 | 0.15-0.3 | |
| EN19 | 0.35-0.45 | 0.1-0.35 | 0.5-0.8 | 0.05 | 0.05 | 0.9-1.5 | 0.2-0.4 | |
| SCM440 | 0.38-0.43 | 0.15-0.35 | 0.6-0.85 | 0.03 | 0.03 | 0.9-1.2 | 0.15-0.3 |
4: 4140 steel mechanical properties
The mechanical properties mainly include tensile strength, yield strength, elongation, area or reduction, hardness, impact value, non-metalic inclusion etc. Different heat treatment, the mechanical properties will be different, such as normalized, tempered, QT. If you want to know the properties, kindly contact the salesman.
5: 4140 steel overviews
| Size | Round | Dia 6-1200mm |
| Plate/Flat/Block | Thickness 6mm-500mm |
|
| Width 20mm-1000mm |
||
| Heat treatment | Normalized ; Annealed ; Quenched ; Tempered | |
| Surface condition | Black; Peeled; Polished; Machined; Grinded; Turned; Milled | |
| Delivery condition | Forged; Hot rolled; Cold drawn | |
| Test | Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. | |
| Payment terms | T/T;L/C;/Money gram/ Paypal | |
| Trade terms | FOB; CIF; C&F; etc.. | |
| Delivery time | 30-45 days | |
| Application | 4140 alloy steels are used for Components, Adapters, Arbors,strippers, holder blocks, mold bases, ejectors, back up and support tooling, fixtures, jigs, molds, cams, drill collars, Axle Shafts, Bolts, Crankshafts,stubs, couplings, reamer bodies, axles, shafting, piston rods, rams, hydraulic machinery shafts, gears, sprockets, gear racks, chain links, spindles, tool bodies, tool holders, tie rods, Connection Rods, Chuck Bodies, Collets, Conveyor Pins & Rolls, Ejector Pins, Forks, Gears, Guide Rods, Hydraulic Shafts & Parts,Lathe Spindles, Logging Parts, Milling Spindles, Motor Shafts, Nuts, Pinch Bars, Pinions, Pump Shafts,boring bars,tracks, slides, wear strips or parts, forming dies, brake dies, trim dies, bolsters, machinery parts and components, etc.. | |
Hot Tags: 4140 hot forged rolled steel round bar, China 4140 hot forged rolled steel round bar suppliers, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes