6m Long 80x40x5mm Ss U Channel Astm A276 Aisi 316l
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 6m long 80x40x5mm ss u channel astm a276 aisi 316l in China. If you're going to wholesale high quality 6m long 80x40x5mm ss u channel astm a276 aisi 316l made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
304 316l Stainless Steel U Channel Size 20x20x2mm
Description
| Products: | Stainless Steel U Channel | Grade: | 201 304 316L |
|---|---|---|---|
| Size: | 3# - 20# | Length: | 6m |
| Type: | Hot Rolled | Service: | Cutting |
| Company: | Factory | Other Materials: | Angle Bar, Square Bar, Hexagon Bar |
| High Light: |
304 u shaped steel bar,316l stainless steel u channel,stainless steel u channel size 20x20x2mm |
||
U-BAR MATERIAL STAINLESS STEEL 304 316L SIZE # 20X20X2MM
U channels are used as trim for hand and stair railings, including escalators, in commercial spaces. Metal railings are easier to maintain and longer-lasting than their plastic or wood counterparts.
Product information:
| Commodity | Stainless Steel U Channel Stainless Steel Hexagonal Bar 304 316 430 202 |
| Grade | 304 316 403 202 |
| Brand | None |
| Certification | SGS,BV,IQI,TUV,ISO,etc |
| Thickness | 2-10mm |
| Size | UPN30-UPN400, UPE80-UPE400,5#--40# |
| Length | 5.8m,6m or customized length |
| Surface | Hot rolled,cold drawn,annealed, pickling |
| Standard | JIS,AISI,ASTM,GB,DIN |
| Delivery time | About15-30 days or based on the sales contract |
| MOQ | 1 TON |
| Advanatages |
Construction field, shipbuilding industry,petroleum, chemical industries, war and electricity industries,food processing and medical industry,boiler heat exchanger,machinery and hardware fields |
Chemical Position:
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo |
| 201 | ≤0.15 | ≤1.00 | 5.5~7.5 | ≤0.060 | ≤0.03 | 3.5~5.5 | 16.00~18.00 | - |
| 202 | ≤0.15 | ≤1.00 | 7.5~10.0 | ≤0.060 | ≤0.03 | 4.0~6.0 | 17.00~19.00 | - |
| 301 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 6.00~8.00 | 16.00~18.00 | - |
| 302 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 8.00~10.00 | 17.00~19.00 | - |
| 304 | ≤0.07 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 8.00~10.00 | 18.00~20.00 | - |
| 304L | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 9.00~13.00 | 18.00~20.00 | - |
| 310S | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 19.00~22.00 | 24.00~26.00 | - |
| 316 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 10.00~14.00 | 16.00~18.00 | 2.00~3.00 |
| 316L | ≤0.03 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 12.00~15.00 | 16.00~18.00 | 2.00~3.00 |
| 321 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 9.00~13.00 | 17.00~19.00 | - |
| 410 | ≤0.15 | ≤1.00 | ≤1.00 | ≤0.040 | ≤0.03 | 11.500~13.50 | - | |
| 430 | ≤0.12 | ≤1.00 | ≤1.00 | ≤0.040 | ≤0.03 | 16.00~18.00 | - |
Physical Property:
| Grade | YS(Mpa) | TS(Mpa) | EL(%) | HV/HB Hardness |
| 304 | ≥205 | ≥520 | ≥40 | ≤200HV |
| 304L | ≥175 | ≥480 | ≥40 | ≤200HV |
| 316 | ≥205 | ≥520 | ≥40 | ≤200HV |
| 316L | ≥175 | ≥480 | ≥40 | ≤200HV |
| 430 | ≥205 | ≥450 | ≥22 | ≤200HV |
| SAF2507 | ≥800 | ≥550 | ≥15 | ≤310HB |
| SAF2205 | ≥620 | ≥440 | ≥25 | ≤290HB |
Surface Finish:
| Surface Finish | Definition | Application |
| 2B | Finished by heat treatment, pickling after cold rolling. Followed by skin pass line to be more brighter and smooth surface | General application Medical instruments, Tableware |
| BA | Bright heat treament after cold rolling | Kitchen utensil, kitchenware, architectural |
| 8K | A mirror-like reflective surface by polishing with finer abrasives over 800mesh | Construction, mirrors, plate sets, decoration elevators |
| HL | Finished by continuous linear polishing | Architectural purpose, Escalators, kitchenware, vehicles |
| NO.1 | Finished by hot rolling, annealing and picking, characterized by white pickled surface | Chemical industry Equipment, industrail tanks |
| NO.4 | Polishing with NO.150 to NO.180 mesh abrasives specified in JISR6001 | Kitchen utensils, Building Construction, Medical equipment |
Packing:

Stainless Steel U Channel Stainless Steel Hexagonal Bar 304 316 430 202 packaging details :
1.with plastic cap to protect both ends
2.weaving bag wrapped outside the pipe
3.then pack into wooden case
The innner size container as below :
1:20ft GP: 5.8m(length) x 2.13m(width) x 2.18m(high) about 24-26CBM ;
2:40ft GP: 11.8m(length) x 2.13m(width) x 2.18m(high) about 54CBM ;
3:40ft HG: 11.8m(length) x 2.13m(width) x 2.72m(high) about 68CBM.
Product Display:
WHY CHOOSE US:
Q1: What is your terms of payment?
A: 30% T/T in advance, the balance 70% before delivery. We will show you the photos of products and package before you pay the balance.
Q2: what is the terms of delivery?
A: FOB, CIF, CFR,
Q3: What is the terms of packing?
A: generally, we pack our goods in bundles or coils with rods or belts, we could also pack the goods as the customers' requirement.
Q4: What is your delivery time?
A: For stocks, we could transport the goods to loading port within 7 days after we received your deposit.
For production period, it usually takes about 15 days-30 days after receiving the deposit.
Q5: Could you produce according to the samples?
A : Yes, we could customer-made by your samples or technique drawings, we could build the mold and fixtures.
Q6: Could you provide the samples?
A: yes, we could provide the free samples on conditons it is available in stocks, however, the the transportation fee is borne by buyer.






Hot Tags: 6m long 80x40x5mm ss u channel astm a276 aisi 316l, China 6m long 80x40x5mm ss u channel astm a276 aisi 316l suppliers, 304 316 Steel Flat Bars With Holes, 420 Stainless H type Steel, Stainless Steel 310S Round Bar, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar