Seamless Carbon Steel Plate Coil HR380F Hot Rolled 3.0mm 1250mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Seamless Carbon Steel Plate Coil HR380F Hot Rolled 3.0mm 1250mm
Description
| Width: | 600-2500mm | Grade: | QStE380TM |
|---|---|---|---|
| Technique: | Hot Rolled | Type: | Steel Plate |
| Standard: | ASTM JIS | Length: | 1000-12000mm |
| Surface Treatment: | Hot Finished | Special Use: | High-strength Steel Plate |
| Thickness: | 1mm-120mm | Surface: | Black Painted |
| Product Name: | Plate | Coil Weight: | 3-10 Tons |
| High Light: |
Seamless Steel Plates Coil,3.0mm Carbon Steel Plate Coil,Hot Rolled Seamless Steel Plates Coil |
||
QStE380TM is a kind of cold formed hot rolled pickled automotive structural steels.QStE380TM is fine grain steel, with good cold formability. QStE380TM High Strength steel coil is used for producing car beams other automotive structural parts, which has the requirements of good cold forming performance and high strength.
QStE380TM HRC chemical composition %
Grade |
C | S | Mn | P | Si | Alt |
| QStE380TM | ≤0.12 | ≤0.025 | ≤1.40 | ≤0.03 | ≤0.35 | ≥0.01 |
QStE380TM steel mechanical properties
Grade |
Yield strength (MPa | Tensile strength (MPa) | Elongation% |
| QStE380TM | 380min | 450-590 | 23min |
QStE380TM delivery condition: HR,AR,Annealing,Aging,Solution
Supply size: thickness 1.2-25mm; coils width 600-2000mm; strips width≦600mm
Product type : QStE380TM steel coil, QStE380TM steel strip,QStE380TM steel sheet
Delivery time : Promptly ( Stock) or 10-40 days (Production)
We keeps more than 10,000 tons in stock each month, including QStE380TM High Strength steel coil and other kinds low carbon steels. Our advantage industry also spread into steel process like : cutting ( any size and any shape ) drilling, welding, milling, machining and steel structure



Hot Tags: seamless carbon steel plate coil hr380f hot rolled 3.0mm 1250mm, China seamless carbon steel plate coil hr380f hot rolled 3.0mm 1250mm suppliers, NI MO corrosion alloy, , nickel chromium molybdenum alloy, monel 401 round bars, nickel chromium iron alloy