Stainless Steel 316H Sheet
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 316h sheet in China. If you're going to wholesale high quality stainless steel 316h sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless steel is divided into various grades. These grades are further subcategorized into high and low versions. Stainless Steel 316H Sheet is one such high carbon alloy that is used in manufacturing sheets. Stainless Steel 316H Plate is said to be reliable and rustproof. These SS 316H Plates offer high yield and tensile strength.

ASTM A240 Type 316H displays augmented carbon content with heat resistance attributes. ASTM A240 Grade 316H also provides good long and short term creeps resistance. 316H 2b Stainless Steel sheets are widely used in chemical, petrochemical, and gas industries.
| Specification | ASTM A240/ ASME SA240 SS 304 |
|---|---|
| Grade | SS 304 (UNS S30400, 1.4301), SS 304L (UNS S30403, 1.4306), SS 310S (UNS S31008, 1.4845), SS 316 (UNS S31600, 1.4401), SS 316Ti (UNS S31635, 1.4571), SS 316L (UNS S31603, 1.4404), SS 317L (UNS S31703, 1.4438), SS 321 (UNS S32100, 1.4541), SS 347 (UNS S34700, 1.455), SS 410 (UNS S41000, 1.4006) |
| Thickness | 4.0mm - 100mm |
| Size | 1000 mm x 2000mm, 1220mm x 2440mm, 4' x 8', 1250mm x 2500mm, 1500mm x 3000mm to 6000mm, 2000mm x 4000mm to 6000mm |
| Finishes | 2D, 2B, 4Pol, BA, X10, XL, Buff, XL Blend S, SATIN (Met with Plastic Coated), NO(8), Hairline, NO.1, NO.4, Mirror Finish |
| Processing | Shearing to Custom Sizes |
A240 GR 316H Rolling Plate also offers superior power at high temperatures. Therefore, SA240 316H Clad Plate is used in pressure vessels and structural functions that work in temperature beyond 500 degrees C. ASTM A240 316H Perforated Plate has a thickness ranging between 4.0 mm to 100 mm.
The density of the AISI 316H EN 1.4404 Rolling Sheet is approximately 8000kg/m3. A240 Tp 316H Hot rolled Plate is made up of a highly alloyed grade of stainless steel. Thus A240 Tp316H Slit Coil can resist corrosion in acids, chlorides, and the alkaline solution even at a raised temperature.

316H Stainless Steel Polished Plateis widely used in heat exchangers, food processing, and brewery equipment, boat fittings, coastal architectural paneling, and so on. ASTM A240 Type 316H Shim Stock is also used in laboratory bench and equipment, mining screens, medical implants, and coastal balustrading.
316H 2b Stainless Steel Flat Sheet requires solution treatment or annealing since it cannot be hardened by heat treatment. 316H Stainless Steel Strip displays excellent fusion welding properties with or without fillers. 316H Stainless Steel Coil is not recommended to undergo oxyacetylene welding.
Hot Tags: stainless steel 316h sheet, China stainless steel 316h sheet suppliers, 400 2 4360 Alloy Pipe, ASTM A240 Grade 431 10mm Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, SS410 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate