1.4162 1.4460 Stainless Steel Pipe
video

1.4162 1.4460 Stainless Steel Pipe

The stainless steel plate has a smooth surface, high plasticity, toughness and mechanical strength, and is resistant to corrosion by acids, alkaline gases, solutions and other media. It is an alloy steel that is not easy to rust, but it is not absolutely rust-free.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4162 1.4460 stainless steel pipe in China. If you're going to wholesale high quality 1.4162 1.4460 stainless steel pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Products Description

1.4162 1.4460 Stainless Steel Pipe

Applications

The main applications are for details with corrosion resistance better than 304L.

LDX 2101 is characterized by:

• Ideal for tank production where corrosion strength is sufficient.
• Good resistance to stress corrosion cracking.
• Good resistance to general corrosion.
• High mechanical strength.
• High resistance to erosion corrosion and corrosion fatigue.

 

Products Properties

 

product-831-375
1.4162 1.4460 Stainless Steel Pipe

Plates Of Middle Thickness

LDX 2101 is a low Ni-alloyed duplex stainless steel with balanced chemistry of chromium, molybdenum and nitrogen content to achieve good resistance to localized and uniform corrosion. The Duplex microstructure contributes to the high strength and high resistance to stress corrosion cracking. Duplex stainless steel have good weldability. Due to risk of embrittlement, LDX 2101 should not be used at temperatures above 250°C. Very price stable high strength alloy.

The steel grade 1.4460 ( also called AISI 329 and SS2324) is a stainless, acid resistant, duplex steel with improved machinability. Since the steel is machinability improved, it is suitable for production of details with comprehensive machining. The steel has very good corrosion resistance particulary in chloride-bearing environments and is extra resistant to pitting corrosion, crevice corrosion, stress corrosion cracking and corrosion fatigue. It also has high strentgth and toughness.

Customer Case

 

 Medium and Thick Plate

FAQ

 

Q: What product information must I provide before purchasing?
A:Please provide the grade, width, thickness, surface treatment requirements and the quantity you require.
Q: What shipping ports are there?
A:We usually ship from Shanghai, Tianjin, Qingdao and Ningbo ports.
Q: What are your payment terms?
A:30% T/T in advance, 70% balance before shipment or based on copy of bill of lading or L/C at sight.
Q: What about product pricing information?
A:Prices vary due to regular changes in raw material prices.
Q: Can I send samples?
A:Of course, we provide free samples and express delivery to customers all over the world.
Q: Do you provide customized product services?
A:Yes, we can produce according to your specifications and drawings.
 

Hot Tags: 1.4162 1.4460 stainless steel pipe, China 1.4162 1.4460 stainless steel pipe suppliers, SS409 Stainless Steel Welded Pipe, 400 2 4360 Alloy Pipe, Corrugated SS Roof Sheet, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, SS410 Stainless Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry