1.4029 1.4021 Stainless Steel Medium Thickness Plate
video

1.4029 1.4021 Stainless Steel Medium Thickness Plate

Provides good ductility when annealed. In a hardened condition, it offers excellent corrosion resistance. Due to added sulfur, renders greatly improved machinability. Chromium steel that can sustain heat treatment.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4029 1.4021 stainless steel medium thickness plate in China. If you're going to wholesale high quality 1.4029 1.4021 stainless steel medium thickness plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Products Description

1.4029 1.4021 Stainless Steel Medium Thickness Plate

Key Features:

  • Excellent machinability properties, due to added sulfur.
  • Similar to type 420, but with free machining properties
  • Provides excellent resistance to corrosion when hardened
  • Can withstand heat treatment
  • Annealed, it provides good ductility
  • Not usually welded, due to hardening properties
  • Only minor cold work operations can be performed because it risks cracking
Products Properties

 

Chemical Composition of 1.4029

C: 0.25 0.32
Si: Max 1.00
Mn: Max 1.50
P: Max 0.04
S: 0.15 0.25
Cr: 12.00 13.50
Ni: Max Min
Mo: Max 0.60

Mechanical Properties of 1.4029

Rp0.2 (MPa) 517 (≥)
Rm (MPa) 724 (≥)
AKV (J) 33
A (%) 31
Z (%) 42
Hardness HBW 333

1.4029 1.4021 Stainless Steel Medium Thickness Plate

medium-thick steel plate

Type 420F stainless steel(1.4029) is chromium, general-purpose steel, which can be heat treated. Due to the addition of sulfur in its composition, it provides greatly improved machinability.Annealed, it offers good ductility. It renders excellent resistance to corrosion in the hardened condition.It is similar to type 420, but stainless-steel type 420F is preferred in applications where good machining properties are required due to complex geometries, such as dental equipment, surgical equipment.

1.4021 is possible to weld and shall be welded with welding consumables similar to that of the parent one. The steel is generally easier to machine than "conventional" austenitic steels. The heat treatment condition of 1.4021 is QT 700 and it should be hot formed in the temperature range 1100-800°C. Slow cooling after hot forming.

Customer Case

 

 Medium and Thick Plate

FAQ

 

Q:what is your delivery time ?
A: Our delivery time is about one week, timing according to the number of customers.

Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.

Q: What is your terms of payment ?
A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable

Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.

Q:Can you send samples?
A:Of course, we can send samples to all parts of the world, our samples are free, but customers need to bear the courier costs.

Hot Tags: 1.4029 1.4021 stainless steel medium thickness plate, China 1.4029 1.4021 stainless steel medium thickness plate suppliers, 400 2 4360 Alloy Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, SS410 Stainless Steel Plate, Corrugated SS Roof Sheet, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate