SS 316L PLATE ASTM A240 316L Stainless Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss 316l plate astm a240 316l stainless steel plate in China. If you're going to wholesale high quality ss 316l plate astm a240 316l stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
In ASTM A240, type 316 and 316L is a chromium nickel austenitic steel, Element molybdenum addition can enhances corrosion resistance of stainless steel, which is the main factor that 316/316l is more corrosion resistant than 304/304l. When 316L steel of low carbon content is only a little higher than 316 steel on strength level. So sometimes grade 316l is almost the same as 316 grade. Another difference, 316l can be used for weld treatment as it contains lower carbon.
316/316L steel has outstanding corrosion resistant properties, whether it is atmospheric or oxidizing environment, even for marine atmosphere, it shows excellent corrosion resistance in welded state. Normally 316/316l steel shows no magnetic in annealed condition, cold drawn or cold rolling process may make it with little magnetic, and it can be fixed with further processing.
316/316L plate is used to manufacture products for applications that are exposed to salt water, acids such as sulfuric acid and chloride, petrochemicals and chemicals and high-heat such as engines and motors.Products include tanks, supports and frames, enclosures and housings, engine, motor and machinery components and parts.
| Chemical Composition of 316/316L steel | ||
|---|---|---|
| Element | 316 | 316L |
| Carbon | 0.08 | 0.030 max |
| Chromium | 16.0-18.0 | 16.0-18.0 |
| Nickel | 10.0-14.0 | 10.0-14.0 |
| Molybdenum | 2.00-3.00 | 2.00-3.00 |
| Manganese | 2.00 | 2.00 |
| Silicon | 0.75 | 0.75 |
| Nitrogen | 0.10 | 0.10 |
| Phosphorus | 0.045 | 0.045 |
| Sulfur | 0.030 |
0.030 |
| Mechanical Property of 316/316l | 316 | 316L |
|---|---|---|
| Yield Strength, min. (ksi) | 30 | 25 |
| Tensile Strength, min. (ksi) | 75 | 70 |
| Elongation, min. (%) | 40 | 40 |
| Hardness, max. (Rb) | 95 | 95 |


FAQ
Q: Can provide OEM/ODM service?
A: Yes. Please feel free to contact us for more details discuss.
Q: How is your Payment Term?
A: Our usual payment methods are T/T, L/C, D/A, D/P, Western Union, Money Gram, payment methods can be negotiated and customized with customers.
Q: Can I get samples before order ?
A: Yes, of course.We can produce by your samples or technical drawings ;
Q: Can I go to your factory to visit?
A: Of course, we welcome customers from all over the world to visit our factory ;
Q:What are the shipping ports?
A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.
Hot Tags: ss 316l plate astm a240 316l stainless steel plate, China ss 316l plate astm a240 316l stainless steel plate suppliers, SS409 Stainless Steel Welded Pipe, ASTM A240 Grade 431 10mm Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, SS410 Stainless Steel Plate, SS431 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates
You Might Also Like
Send Inquiry