CCS EH32 Ship Steel Plate , ABS DNV Marine Steel Plate
video

CCS EH32 Ship Steel Plate , ABS DNV Marine Steel Plate

ASTM A131 DH32 steel for shipbuilding is not only the high tensile strength steel but also is the Hull structural steel with good toughness properties, higher strength,strong corrosion-resistance,the processing properties,and good welding properties.Shipbuilding steel grade DH32 is used for shipbuilding and oil platform purpose and they are approved by ABS,DNV,GL,BV,LR,NK,RINA and other classification societies.What's more, DH32 shipbuilding steel plate can be used in manufacturing the ship's hull structure whose weight is below 10000 tons.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ccs eh32 ship steel plate , abs dnv marine steel plate in China. If you're going to wholesale high quality ccs eh32 ship steel plate , abs dnv marine steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

CCS EH32 ship steel plate , ABS DNV marine steel plate

Description

Name: Ship Steel Plate Material: A D E F Grade
Length: 6-11m Width: 1500-2500mm
Thickness: 5-250mm Type: Hot Rolled
High Light:

shipping plate

,

shipbuilding steel plate

Ship building plate / CCS EH32 ship steel plate, EH32 steel plate, ABS DNV steel plate

The EH32 shipbuilding steel plate is the mainly kinds of steel for shipbuilding and oil platform, the shipbuilding gradeEH32 can be used in the manufacture of the ship's hull structure, whose weight is more then 10000 tons. Shipbuilding grade EH32 is the high tensile strength steel, EH32 steel for shipbuilding and oil platform must be good toughness properties, higher strength, strong corrosion-resistance, the processing properties, and welding properties.

 

EH32 shipbuilding steel plate Chemical Composition %


Grade

C max

Si max

Mn

P max

S max

Als min

Ti max

Cu max

Cr
max

Ni
max

Mo
max

EH32

0.18

0.50

0.90-1.60

0.035

0.035

0.015

0.02

0.35

0.20

0.40

0.08

 

EH32 shipbuilding steel plate Mechanical Property


Grade

Rm
(MPa)

Re(MPa) min

A% min

Akv/J min

EH32

440-570

315

22

E.T °C

Thickness (mm)

-40

50

>50-70

>70-100

L

C

L

C

L

C

31

22

38

26

46

31

 

EH32 shipbuilding steel plate Condition Of Delivery


Grade

Fine grains elements

category

The thickness of steel

≤ 12

>12.5-20

>20-25

>25-35

>35-50

>50-100

EH32

Any

Plate/sheet

N,TM

Profile steel

N(25),TM(25),AR*(15),CR*(15)

-

Note: 1. delivery condition: A =Any ; N=Normalized ; CR=Control Rolled ; TM=TMPC, Temperature - deformation control rolling; AR*= Can be hot rolled with the agreement of Classification Society ; CR*=Can be control rolled with the agreement of Classification Society .


2. The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.

EH32 shipbuilding steel plate Contrast in the different standard


ASTM A131M

TOCT 5521

JIS G3106

BS LR

GB712

EH32

E32

SM490B
SM490C

EH32

E32

 

 

Application

1)Petroleum, Chemical enterprise, superheater of boiler,
heat exchanger
2)High temperature resistant transmission fluid pipe
in power station
3)Ship with pressure pipe
4)The exhaust purification devices
5)Home appliance, electrical components, decorate pipe
6)Precision instrument manufacture

CCS EH32 ship steel plate , ABS DNV marine steel plate 0CCS EH32 ship steel plate , ABS DNV marine steel plate 1

 

Hot Tags: ccs eh32 ship steel plate , abs dnv marine steel plate, China ccs eh32 ship steel plate , abs dnv marine steel plate suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, Corrugated SS Roof Sheet, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 400 2 4360 Alloy Pipe