DNV Grade A36 Hot Rolled Ship Steel Plate 7000-12000mm Length
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of dnv grade a36 hot rolled ship steel plate 7000-12000mm length in China. If you're going to wholesale high quality dnv grade a36 hot rolled ship steel plate 7000-12000mm length made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
DNV grade A36 hot rolled ship steel plate 7000-12000mm length
Description
| Name: | Ship Steel Plate | Material: | A D E F Grade |
|---|---|---|---|
| Length: | 6-11m | Width: | 1500-2500mm |
| Thickness: | 5-250mm | Type: | Hot Rolled |
| High Light: |
shipbuilding steel plate,marine steel plate |
||
Specifications
abs a36 ship steel plate
Famous Domestic Mills: Wisco,Baosteel etc.
Offer with Mill's Test Certificate
DNV ABS grade A36 Ship steel plate, hot rolled ship steel plate A36
1. Steel Grade:
|
Material |
Steel |
|
Thickness |
6-38mm |
|
Width |
1800-3200mm |
|
Length |
7000-12000mm |
|
Executive standard |
ASTM, GB, JIS |
|
Grade |
A,B,D, E ,AH32, AH36,DH32,DH36, EH32,EH36 |
|
Usage |
Ship building, construction, light industry, household appliance, automobile |
|
Manufacturer process |
Hot rolled |
|
Packing |
Properly packed for ocean freight exportation in containers |
|
Notice |
special design available is according to the requirement of customers |
2. Hardness and Mechanical Properties
|
Mechanical Properties |
|||||||||
|
Grade |
Thickness (mm) |
Yieldpoint (Mpa) |
Tensile Strength (Mpa) |
Elongation (%)≤ |
Impact test |
Cold Bend Test |
|||
|
Temperature (0C) |
Average AKV A KV/j |
b=2a 1800 |
b=5a 1200 |
||||||
|
lengthways |
crosswise |
||||||||
|
≥ |
|||||||||
|
A |
≤50 |
235 |
400~490 |
22 |
/ |
/ |
/ |
d=2a |
/ |
|
B |
0 |
27 |
20 |
/ |
d=3a |
||||
|
D |
-10 |
||||||||
|
E |
-40 |
||||||||
|
AH32 |
≤50 |
315 |
440~590 |
22 |
0 |
31 |
22 |
/ |
d=3a |
|
DH32 |
-20 |
||||||||
|
EH32 |
-40 |
||||||||
|
AH36 |
≤50 |
355 |
490~620 |
21 |
0 |
34 |
24 |
/ |
d=3a |
|
DH36 |
-20 |
||||||||
|
EH36 |
-40 |
||||||||
Classification Society: ABS,BV,CCS,DNV,GL,KR,LR,NKK,RINA
3. Application
It has been widely used in ship building, construction, light industry, household appliance, automobile.
4. Shipment Information
|
MOQ: |
25 Metric Ton/Metric Tons |
|
Package: |
bulk packing with steel belt or customer required |
|
Trade terms: |
FOB, CFR, CIF |
|
Payment method: |
L/C,D/A,D/P,T/T,Western Union |
|
Port of Loading: |
Any port in China |
|
Delivery Time: |
15 days from ordering date |
If you have special requirement, Welcome to contact us.
5. Advantage of us
best price
good quality
warm service
fast deliver
sale in stock
near Shanghai Port


Hot Tags: dnv grade a36 hot rolled ship steel plate 7000-12000mm length, China dnv grade a36 hot rolled ship steel plate 7000-12000mm length suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS410 Stainless Steel Plate, 400 2 4360 Alloy Pipe, SS409 Stainless Steel Welded Pipe, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Corrugated SS Roof Sheet
You Might Also Like
Send Inquiry